MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Garlock Klozure® Mill-Right® N NBR Oil Seal
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: A proprietary formulation of Nitrile (NBR). Engineered specifically for high-performance applications that demand the tightest sealing system, longest service life, and constant operation within harsh chemical environments.

Information provided by Garlock Rubber Technologies

Key Words: nitrile, butadiene acrylonitrile
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80
Coefficient of Friction 1.788
Taber Abrasion, mg/1000 Cycles 150ASTM D4060
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 200 °FContinuous
 250 °FSpike
Minimum Service Temperature, Air -40.0 °F
 
Processing PropertiesOriginal ValueComments
Shelf Life 60.0 Month
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Nitrile Rubber (NBR, Acrylonitrile-Butadiene Rubber)
Garlock Klozure® Mill-Right® ES HNBR Oil Seal
Nitriflex NitriClean 2858 NBR - Nitrile Rubber
Seals Eastern 5488 Nitrile Rubber
ATG s.r.l. XNBR Carboxylated Nitrile Rubber

PGARL996 / 157544

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.