MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Vacupor® NT Porextherm
Categories: Ceramic

Material Notes: Vacupor® NT is a microporous insulation material which has an extremely low thermal conductivity coefficient giving it very good insulating properties. Vacupor® NT consists of inorganic oxides. The main constituent is fumed silica, the other components are opacifiers for minimizing infrared radiation, and silicates. Vacupor® NT (core material) is not flammable and meets the requirements of IMO FTPC part 1 and DIN ISO 4102 part 1, A1. Vacupor® NT is heat sealed under vacuum in a multilayer vacuum metalized film. The very low internal pressure and the microporous panel core enable it to reach extremely low thermal conductivity values.

Application: Vacupor® NT was specially developed for applications in vacuum insulation technology. The low density and the specially developed IR opacifiers contained in these grades greatly reduce the thermal conductivity of Vacupor® NT Systems.

Typical applications: Vacupor® NT is also successfully used as insulation material in the following areas:

  • Domestic appliances (refrigerator and freezer cabinets)
  • Absorption refrigerators
  • Cryogenic freezer
  • Temperature controlled packaging
  • Transport boxes
  • Facade elements
  • Terrace insulation
  • Cold storage floor insulation
.

Information provided by Morgan Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.50 - 3.00 g/ccdependent on board thickness
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity <= 0.00500 W/m-Kat 1 mbar, dependent on the panel size and thickness, internal pressure can be between 0.5-5mbar. The standard internal pressure in the evacuation chamber is <0.5mbar
 <= 0.0190 W/m-Kat ambient pressure
 0.00363 W/m-K
@Pressure <=1.00 MPa
 0.00366 W/m-K
@Pressure 0.0000100 MPa
 0.00375 W/m-K
@Pressure 0.000100 MPa
 0.00425 W/m-K
@Pressure 0.00100 MPa
 0.00870 W/m-K
@Pressure 0.0150 MPa
 0.0183 W/m-K
@Pressure 0.100 MPa
Maximum Service Temperature, Air <= 120 °CThe limits are fixed by the barrier film (sealing material) used; constant load: =<80°C; short load time with 120°C, roughly 30minutes.
Minimum Service Temperature, Air >= -50.0 °C
 
Descriptive Properties
Colorsilver

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
MarkeTech Silica Aerogel
Industrial Nanotech Nansulate™ High Heat Translucent Insulation Coating
Sharadaa Ceramics Resin Bonded Slabs
Unifrax Excelfrax® 1800 Flexliner Microporous Insulation
Overview of materials for Epoxy/Carbon Fiber Composite

CMORF6001 / 202785

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.