MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Washington Penn H2GF3 Polypropylene, 30% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Glass Fiber Filler

Material Notes: Homopolymer. Excellent heat aged physical properties.

Applications: Under hood applications, battery trays, exercise equipment

Data provided by Washington Penn Plastic Co., Inc.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.12 g/ccASTM D792
Melt Flow 5.0 g/10 min
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 76.0 MPaASTM D638
Flexural Yield Strength 48.0 MPaASTM D790
Flexural Modulus 5.00 GPaTangent; ASTM D790
Izod Impact, Notched 0.900 J/cm
@Thickness 3.17 mm
ASTM D256
Izod Impact, Unnotched 3.20 J/cm
@Thickness 3.17 mm
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 144 °CASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Washington Penn Polypropylene Copolymer 30% Glass Reinforced
Washington Penn PPH2UFO Polypropylene, Unfilled
Overview of materials for Polypropylene, Molded
Washington Penn Homopolymer Polypropylene 20% Glass Reinforced
Washington Penn Polypropylene Copolymer 20% Glass Reinforced, 15 MFI

PWPP00 / 72783

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.