MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Cosmic Plastics D69/6130 Long Glass Fiber Filled Diallyl Iso-Phthalate Molding Compound  (discontinued **)
Categories: Polymer; Thermoset; Diallyl Phthalate (DAP); Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled

Material Notes: Description: Cosmic D69 / 6130 is a long glass fiber filled, general purpose diallyl ortho phthalate molding compound which is supplied in a flake form. It can be easily molded in compression or transfer equipment and can be readily preformed for ease in handling. It can be stored at room temperature for two years without reducing performance.

Features: D69 / 6130 combines the advantages of high impact strength, high insulation resistance, excellent compressive and flexural strength, and easy moldability.

Applications: Structural parts, housings, terminals and insulators, or other applications requiring strength.

Information provided by Cosmic Plastics Inc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.72 g/cc
Bulk Factor 6.0
Water Absorption 0.30 %
@Temperature 50.0 °C,
Time 173000 sec
Linear Mold Shrinkage 0.0010 - 0.0040 in/in
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 6000 - 10000 psi
Flexural Strength 13000 - 17000 psi
Compressive Strength 24000 - 30000 psi
Izod Impact, Notched 3.00 - 6.00 ft-lb/in
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+16 ohm-cm
 5.00e+10 ohm-cm
@Temperature 70.0 °C,
Time 2.59e+6 sec
100% RH
Surface Resistance >= 1.00e+16 ohm
 5.00e+10 ohm
@Temperature 70.0 °C,
Time 2.59e+6 sec
100% RH
Dielectric Constant 3.9
@Frequency 1e+6 Hz
Dry
 4.0
@Frequency 1000 Hz
Dry
 4.1
@Frequency 1e+6 Hz
Wet
 4.2
@Frequency 1000 Hz
Wet
Dielectric Strength 360 V/milWet, step by step
 400 V/milDry, step by step
Dielectric Breakdown 60 VWet, step by step
 62 VDry, step by step
Dissipation Factor 0.0060
@Frequency 1000 Hz
Dry
 0.0090
@Frequency 1000 Hz
Wet
 0.013
@Frequency 1e+6 Hz
Dry
 0.015
@Frequency 1e+6 Hz
Wet
Arc Resistance 180 sec
 
Thermal PropertiesOriginal ValueComments
CTE, linear 24.0 µm/m-°C
@Temperature -40.0 - 100 °C
Heat Distortion Temperature 260 °C
 
Processing PropertiesOriginal ValueComments
Mold Temperature 135 - 190 °C
 
Descriptive Properties
Dimensional Stability<0.01%
MIL-M-14GDI-30ASTM D5948-96
Molding Pressure500-8000 psi
Water Extract Conductance.00003 mhow/cm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Zenite® 6130 WT010 30% GF LCP (Extended Tabular Temperature Data)
Celanese Zenite® 6130 BK010 LCP, 30% glass reinforced (Extended Tabular Temperature Data)
Universal Wire Works 6130 (AMS 6462) Low Alloy Steel Welding Wire
Sumitomo Bakelite RX® 643 Phenolic Resole Compound
Cosmic Plastics 6130 Long Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound

PCOSM007 / 190789

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.