MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Lord Adhesives Circalok™ E-105 Clear/Circalok 6250 B Epoxy System
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: LORD® E-105 Clear/Circalok™ 6250 epoxy system is a two-component system designed for use in applications requiring high fluidity, such as epoxy-fiberglass laminations; sealing, impregnating and see-through castings. Handling and cured properties of the two-component epoxy system are dependent on the hardener used with LORD E-105 Clear epoxy resin.

Features: provides good adhesion to laminate surfaces. cured system provides excellent resistance to chemicals. cures to a semi-rigid system; provides excellent impact resistance, suitable for use in large castings.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.940 g/ccEP-6250 Hardener
 1.13 g/cc
@Temperature 25.0 °C
E-105 Resin
Water Absorption 0.20 %cured
Viscosity 350 cP
@Temperature 25.0 °C
EP-6250 Hardener
 600 cP
@Temperature 25.0 °C
E-105 Resin, RVT, Spindle 5, 100 rpm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 90cured
Tensile Strength 8300 psi
@Temperature 25.0 °C
cured
Elongation at Break 4.6 %cured
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cm
@Temperature 25.0 °C
cured
Dielectric Constant 4.0
@Frequency 1e+6 Hz,
Temperature 25.0 °C
cured
Dissipation Factor 0.020
@Frequency 1e+6 Hz,
Temperature 25.0 °C
cured
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 hour
@Temperature 65.0 °C
 24.0 hour
@Temperature 25.0 °C
Working Life 120 - 180 min
@Temperature 25.0 °C
Mixed
Shelf Life 12.0 Month
@Temperature 25.0 °C
E-105 Resin, from date of manufacture in original, unopened container
 12.0 Month
@Temperature 25.0 °C
EP-6250, from date of manufacture in original, unopened container
 
Descriptive Properties
AppearanceAmber LiquidEP-6250
 Clear LiquidE-105 Resin
Mix Ratio100 to 50Resin to hardener, by weight
 100 to 58Resin to hardener, by volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLORD9283 / 232639

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.