MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Shakespeare Isocor™ CU145SI Nylon 6/66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, Unreinforced

Material Notes: Isocor™ CU145SI is a high viscosity, plasticized, PA-6/66 copolymer resin. This resin is specifically suited for applications requiring excellent abrasion resistance while maintaining a balance of properties including chemical resistance and flexibility. This resin can be processed using conventional techniques.

Used for grass trimmer line and cable jacketing.

Information provided by Shakespeare Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.11 g/ccASTM D 792
Water Absorption 0.49 %24 hour immersion; ASTM D 570
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 5600 psiASTM D 638
Tensile Modulus 280000 psiASTM D 638
Izod Impact, Notched 1.90 ft-lb/inASTM D 256
 
Thermal PropertiesOriginal ValueComments
Melting Point 194 °CDSC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
EMS-Grivory Grilon® TSC-10/4 EC black 9832 PA666-CF
Shakespeare Isocor™ HG20SC Nylon 612
Shakespeare Isocor™ CF140ZI Nylon 6/66
BASF Ultramid® C33 01 PA66/6 (Dry)
Shakespeare Isocor™ SVP4011 high viscosity PA-6/69

PSHAKE117 / 67396

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.