MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

(Viewing data as-entered. Click here to return)
Aluminum A390.0-T6, Permanent Mold Cast
Categories: Metal; Nonferrous Metal; Aluminum Alloy; Aluminum Casting Alloy

Material Notes:

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: AAA390.0-T6; UNS A13900; Aluminium A390.0-T6; AlA390.0-T6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.72 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 145500 kg load, 10 mm ball
Hardness, Knoop 184Estimated from Brinell Hardness.
Hardness, Rockwell A 53Estimated from Brinell Hardness.
Hardness, Rockwell B 86Estimated from Brinell Hardness.
Hardness, Vickers 169Estimated from Brinell Hardness.
Tensile Strength, Ultimate 310 MPa
Tensile Strength, Yield 310 MPa
@Strain 2 %
Elongation at Break <= 1.0 %in 50 mm
Tensile Modulus 81.2 GPa
Compressive Modulus 82.8 GPa
Fatigue Strength 115 MPa
@# of Cycles 5.00e+8
Notch Status unknown, R.R. Moore Test
Machinability 10 %0-100 Scale (100=best)
Shear Strength 187 MPaCalculated
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000640 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 389 J/gTypical for cast aluminum
CTE, linear 18.0 µm/m-°C
@Temperature 20.0 - 100 °C
 22.5 µm/m-°C
@Temperature 20.0 - 300 °C
Estimated by MatWeb from similar alloys
Specific Heat Capacity 0.963 J/g-°CTypical for cast aluminum
Thermal Conductivity 134 W/m-K
Melting Point 507 - 649 °C
Solidus 507 °C
Liquidus 649 °C
 
Processing PropertiesOriginal ValueComments
Solution Temperature 925 °F
Aging Temperature 350 °Fhold at temperature for 8 hrs
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 75.2 - 79.6 %As remainder
Copper, Cu 4.0 - 5.0 %
Iron, Fe <= 0.50 %
Magnesium, Mg 0.45 - 0.65 %
Manganese, Mn <= 0.10 %
Other, each <= 0.10 %
Other, total <= 0.20 %
Silicon, Si 16 - 18 %
Titanium, Ti <= 0.20 %
Zinc, Zn <= 0.10 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 354.0-T62, Permanent Mold Cast
Aluminum A390.0-T6 Sand Cast
Aluminum A390.0-T7, Permanent Mold Cast
Aluminum 242.0-T61, Permanent Mold Cast
Aluminum A390.0-F, -T5, Permanent Mold Cast

MAC3900A6P / 10053

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.