MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sunoco TI5600M Polypropylene High Crystallinity Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Market Segment: Compounding

Suggested Uses Include Compounding

Information provided by Sunoco Chemicals.

Braskem acquired Sunoco Chemicals polypropylene product line in 2010.

Key Words: Highly Crystalline Homopolymer Phase, Very High Molecular Weight EPR Phase, Very High Flexural Modulus
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 66 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 4900 psi2 in/min, 50 mm/min; ASTM D638
Elongation at Yield 5.0 %2 in/min, 50 mm/min; ASTM D638
Flexural Modulus, 1% Secant 240000 psi0.05 in/min, 1.3 mm/min; ASTM D790A
Izod Impact, Notched 0.900 ft-lb/inASTM D256A

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Melos® FM 958 Ethylene Propylene Rubber (EPR)
Kraton® G1765X (EP)n Multi-Arm Copolymer
Kraton® G1750X (EP)n Multi-Arm Copolymer
Kraton® D4270 J (O/E SBS) Branched Block Copolymer
Kraton® D4153 E (O/E SBS) Linear Block Copolymer

PSUN59 / 69378

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.