MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M Novec™ 1230 Fire Protection Fluid
Categories: Fluid

Material Notes: 3M™ Novec™ 1230 Fire Protection Fluid is a halon and HFC clean agent replacement technology, designed to alleviate concerns for human safety, performance and the environment.

Features and Benefits:

  • Next generation halon and HFC clean agent replacement technology
  • Zero ozone depletion potential
  • 5-day atmospheric lifetime
  • Global warming potential of 1
  • Largest margin of safety among chemical clean agents for occupied spaces

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.60 g/cc0.0578 lb/in³Sat. Liquid
Viscosity Measure  0.39 cSt
@Temperature 25.0 °C
0.39 cSt
@Temperature 77.0 °F
Liquid
 0.56 cSt
@Temperature 0.000 °C
0.56 cSt
@Temperature 32.0 °F
Liquid
Molecular Weight 316.04 g/mol316.04 g/mol
Vapor Pressure 0.404 bar303 torr
 
Chemical PropertiesMetricEnglishComments
Critical Pressure 18.65 bar13990 torr
Critical Temperature 168.7 °C335.7 °F
Critical Density 0.639 g/cc0.0231 lb/in³
Critical Molar Volume 494.5 cm³/mol30.18 in³/mol
 
Thermal PropertiesMetricEnglishComments
Heat of Vaporization 88.0 J/g
@Temperature 49.2 °C
37.9 BTU/lb
@Temperature 121 °F
Specific Heat Capacity 1.103 J/g-°C0.2636 BTU/lb-°FLiquid
 0.0987 J/g-°C
@Pressure 0.101 MPa
0.0236 BTU/lb-°F
@Pressure 14.7 psi
Vapor
Boiling Point 49.2 °C
@Pressure 0.101 MPa
121 °F
@Pressure 14.7 psi
 
Descriptive Properties
Relative Dielectric Strength2.31 atm (N2=1.0)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Novec™ 612 Magnesium Protection Fluid
3M Novec™ 7100 Engineered Fluid
3M Novec™ 7000 Engineered Fluid
3M Fluorinert™ FC-72 Electronic Liquid
3M Novec™ 649 Engineered Fluid

PMM33118 / 167865

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.