MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Excalibar ExCal® CW 325 Calcium Carbonate CaCO3 Powder
Categories: Ceramic; Other Engineering Material; Additive/Filler for Polymer

Material Notes: ExCal® CW calcium carbonate products are processed from a high-purity ore, to exacting specifications at the Houston, Texas plant. These grades are processed for use in plastics, rubber, coatings, adhesives, sealants, mastics, and other specialty applications where color, binder demand and economics are of importance.

Information provided by Excalibar Minerals LLC.

Key Words: CaCO3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.70 g/cc
Bulk Density 53.0 lb/ft³Loose
 88.0 lb/ft³Packed
Brightness 96 %Hunter Dry Brightness, L Value
Oil Absorption 14 %
Moisture Absorption 0.1 %
Particle Size 14 µmMedian
Particle Mesh Size 325 Mesh97% Passes
pH 7 - 8
 
Component Elements PropertiesOriginal ValueComments
Al2O3 0.95 %
Fe2O3 0.050 %
SiO2 <= 0.010 %
 
Descriptive Properties
Acid Solubility98
CaCO3 wt%98
MgCO3 wt%0.8
R2O3 wt%0.1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CIMBAR Crescent 12 Calcium Carbonate (CaCO3), Fine Powder
CIMBAR Crescent 50 Calcium Carbonate (CaCO3), Coarse Powder
CIMBAR RiverCal™ 8107 & 8107C Calcium Carbonate (CaCO3)
CIMBAR Crescent 35 Calcium Carbonate (CaCO3), Medium Powder
Excalibar ExCal® 200 Calcium Carbonate CaCO3 Powder

CEXCAL981 / 176048

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.