MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Advanced Elastomer Systems Santoprene® 8281-75 Thermoplastic Rubber  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other melt processing techniques. Supplied as free-flowing pellets in 25 kilogram (55 pound) moisture barrier bags.

Features:

  • Non-hygroscopic product, requires little to no drying before processing
  • Neutral, easy coloring formulation
  • USP Class VI Certificate of Compliance
  • Drug Master File established with FDA

Product Notes: Values are for injection molded plaques, side gated.
82.6 mm x 117.5 mm x 3 mm

Information provided by Advanced Elastomer Systems.

Advanced Elastomer Systems is now a part of ExxonMobil. This grade was removed from the Advanced Elastomers Systems standard product line before the ExxonMobil acquisiton.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.920 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 755 seconds; ASTM D2240
 805 seconds, After oven air aging 168 hours @ 150°C; ASTM D2240
Tensile Strength at Break 783 psiAfter oven air again 168 hrs. @ 150°C; ASTM D412
 870 psiAcross flow; ASTM D412
Tensile Strength, Yield 580 psiAt 100% elongation, across flow; ASTM D412
Elongation at Break 292.5 %After oven air aging 168 hrs. @ 150°C; ASTM D412
 450 %Across flow; ASTM D412
Tear Strength 200 pli73°F; ASTM D624
Compression Set 28 %
@Temperature 22.8 °C,
Time 612000 sec
Method B; ASTM D395
Tensile Set 25 %ASTM D412
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -76.0 °FASTM D746
 
Processing PropertiesOriginal ValueComments
Processing Temperature 177 - 232 °C
Drying Temperature 82.0 °CDesiccant Dryer
Dry Time 3 hourDesiccant Dryer
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Advanced Elastomer Systems Santoprene® 8281-90 Thermoplastic Rubber
ExxonMobil Santoprene® 8281-75MED Thermoplastic Elastomer
Advanced Elastomer Systems Santoprene® 181-55 Thermoplastic Rubber
Advanced Elastomer Systems Trefsin® 3101-75 W305 Thermoplastic Rubber
ExxonMobil Santoprene® 8281-90MED Thermoplastic Elastomer

PADW167 / 22885

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.