MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay RHODOLINE® 581B Surfactant
Categories: Fluid

Material Notes: Description: Mineral oil defoamers for high PVC systems

Chemical Name: DEFOAMER

CAS: 64742-47-8

Available in: Asia Pacific, Europe, Latin America and North America

Solubility(2% in DI Water): Coarse Dispersion, RP-0547

Applications: The amount of RHODOLINE© 581B required for a specific application should be determined in each case, because of the variance in factors creating foam. Since severe foaming is often controlled with 0.1% RHODOLINE© 581B, this concentration is suggested as a starting point. Make subsequent adjustments to dilute or increase the concentration to the most efficient and economical strength. In some applications, higher concentrations will be needed to obtain the desired persistence. RHODOLINE© 581B will separate on prolonged standing; therefore, it should be mixed well before using. For greater efficiency and stability, an emulsion pre-mix is suggested. This is prepared by adding with mixing one part of water to two parts of RHODOLINE© 581B. More dilute emulsions may be used; however, they require more frequent mixing before use.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.790 - 0.830 g/ccRP-17617
pH 4.5 - 6.52% Solution; RP-0420
 6.0 - 6.7Acid Value; RP-9187
Viscosity <= 1000 cP#3 sp @ 60 rpm; RP-0596
Brookfield Viscosity 500 cP30 rpm
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
AppearanceHazy Cream LiquidRP-0064

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay RHODOLINE® 622 Surfactant
Solvay RHODOLINE® DF-988 Surfactant
Solvay RHODOLINE® LC-2 Surfactant
Solvay RHODOLINE® DF-665 Surfactant
Solvay RHODOLINE® 681-F Surfactant

WRHOD477 / 137708

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.