MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Copper Alloy, UNS C19240, H01 Temper, Flat Products
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Extra Spring

Fabrication Properties: Excellent Suitability – Soldering, Brazing; Good Suitability – Capacity for Being Cold Worked; Fair Suitability – Spot Weld, Seam Weld, Butt Weld, Capacity for Being Hot Formed

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.322 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 86.0 ksiTypical
 73.0 - 106 ksi
Tensile Strength, Yield 83.0 ksi0.2% Offset, Typical
 70.0 - 104 ksi0.2% Offset
Elongation at Break >= 5.0 %
Tensile Modulus 17600 ksi
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000340 ohm-cm50% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.70 µin/in-°F
@Temperature 20.0 - 200 °C
Thermal Conductivity 118 BTU-in/hr-ft²-°F
Melting Point <= 1974 °F
Liquidus 1974 °F
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu >= 97.5 %
Iron, Fe 0.15 - 0.45 %
Lead, Pb <= 0.020 %
Manganese, Mn <= 0.020 %
Phosphorus, P 0.040 - 0.20 %
Silicon, Si <= 0.010 %
Tin, Sn <= 0.80 %
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC19240x2 / 291750

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.