MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Beijing Evergrow Resources ASHRAE HEPA ULPA-K19 Glass Fiber Paper
Categories: Ceramic; Glass; Glass Fiber

Material Notes: Fiber made from melted glass that is drawn into a thin fiber less than a thousandth of an inch in diameter. The fiber may be spun into threads and woven into fabrics which suitable for many applications ,such as removal of micron and submicron size particulates from both liquids and gases,or used in an acoustic, electrical, or thermal insulating material.
    Features:
  • Lightness, heat resisting, low thermal capacity and low thermal conductivity, soft and excellent fire-isolation.
  • Anti-heat energy and heat stability.
  • Anti-mildew, anti-insect, un-scattered and good stretching resistance.
  • Excellent anti-ageing.
  • Excellent sound absorbability, adsorption and filtering.
  • It can be cut, sewn according to requirements and it's also easy to construct.

Information provided by Beijing Evergrow Resources.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 290 - 350 microns
 
Descriptive Properties
Air Resistance (Pa)<= 18
Efficiency (%)>= 90
Mark 0.3 Micron Air Flow Rate (L/min-ºC)0.06
Tensile Strength at Yield (N/m)120CD
 160MD
Weight (g/m²)65

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Isoflon Tisoflon® 3 AD Polytetrafluoroethylene Coated Glass Fabric
Isoflon Tisoflon® 6 AD EXTRA SMOOTH Polytetrafluoroethylene Coated Glass Fabric
Hexcel® HexForce™ 104 Fiber Glass Fabric
Isoflon Tisoflon® 10 AD Polytetrafluoroethylene Coated Glass Fabric
Isoflon Tisoflon® 5 AD Polytetrafluoroethylene Coated Glass Fabric

PBEIJ085 / 90154

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.