MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Röchling SUSTARIN® H AF - DE588 POM/Acetal Homopolymer
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Homopolymer, Unreinforced

Material Notes:
  • Good dimensional stability
  • Very good sliding properties
  • Very wear resistance
Product applications:
  • Mechanical engineering
  • Electrical industry
  • Materials handling industry
Produced from DuPont Delrin® AF-DE588 acetal.

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.54 g/ccASTM D792
Water Absorption 0.80 %ASTM D570
 0.20 %
@Time 86400 sec
ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 50ASTM D785
Hardness, Rockwell R 110ASTM D785
Hardness, Shore D 76ASTM D2240
Tensile Strength, Yield 6630 psiASTM D638
Elongation at Break 30 %ASTM D638
Tensile Modulus 540000 psiASTM D638
Flexural Strength 12500 psiASTM D790
Flexural Modulus 405000 psiASTM D790
Compressive Strength 12600 psiASTM D695
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 1.00e+16 ohmASTM D257
Dielectric Constant 3.1
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 15.7 kV/mmASTM D149
Dissipation Factor 0.0090
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 44.0 µin/in-°FASTM D696
Thermal Conductivity 2.00 BTU-in/hr-ft²-°F
Melting Point 350 °F
Maximum Service Temperature, Air 185 °F
Deflection Temperature at 0.46 MPa (66 psi) 334 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 244 °FASTM D648
Flammability, UL94 HB
@Thickness 3.17 mm
 
Compliance PropertiesOriginal ValueComments
FDA No
NSF No
USDA No

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Stat-Tech™ AT-CB2/000 CR Acetal (POM) Copolymer
Avient Lubri-Tech™ AT-15GP/5T Acetal-Copolymer, PTFE Lubricated
Polyram RamTal PMH2022 Polyacetal Homopolymer for Injection Molding
Murtfeldt Murytal® H Acetal Homopolymer
Mitsubishi Iupital® TC3015 Copolymer Acetal

PROCH9035 / 232738

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.