MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 0.890 - 1.50 g/ccAverage value: 1.06 g/cc Grade Count:226
Water Absorption 0.0500 - 1.00 %Average value: 0.560 % Grade Count:24
Moisture Absorption at Equilibrium 0.200 - 0.250 %Average value: 0.208 % Grade Count:12
Maximum Moisture Content 0.0100 - 0.0500Average value: 0.0262 Grade Count:45
Linear Mold Shrinkage 0.00200 - 0.00900 cm/cmAverage value: 0.00556 cm/cm Grade Count:191
Linear Mold Shrinkage, Transverse 0.00200 - 0.00800 cm/cmAverage value: 0.00610 cm/cm Grade Count:23
Melt Flow 0.200 - 43.0 g/10 minAverage value: 7.23 g/10 min Grade Count:231
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 96.0 - 119Average value: 109 Grade Count:146
Ball Indentation Hardness 85.0 - 115 MPaAverage value: 103 MPa Grade Count:28
Tensile Strength, Ultimate 19.6 - 63.0 MPaAverage value: 44.1 MPa Grade Count:83
Tensile Strength, Yield 33.0 - 170 MPaAverage value: 47.5 MPa Grade Count:166
Elongation at Break 2.50 - 70.0 %Average value: 21.8 % Grade Count:127
Elongation at Yield 2.10 - 10.0 %Average value: 3.42 % Grade Count:58
Modulus of Elasticity 1.70 - 2.70 GPaAverage value: 2.29 GPa Grade Count:64
Flexural Yield Strength 45.6 - 142 MPaAverage value: 73.0 MPa Grade Count:180
Flexural Modulus 1.73 - 6.86 GPaAverage value: 2.39 GPa Grade Count:201
Poissons Ratio 0.380 - 0.400Average value: 0.388 Grade Count:15
Izod Impact, Notched 0.392 - 4.27 J/cmAverage value: 1.74 J/cm Grade Count:110
 0.5339 - 1.60 J/cm
@Temperature -40.0 - 0.000 °C
Average value: 0.983 J/cm Grade Count:7
 0.400 - 1.65 J/cm
@Temperature -40.0 - 0.000 °C
Average value: 0.983 J/cm Grade Count:6
 0.400 - 1.65 J/cm
@Thickness 3.17 - 12.7 mm
Average value: 0.983 J/cm Grade Count:6
Izod Impact, Unnotched 0.392266 - 1.27486 J/cm
@Temperature -30.0 - -30.0 °C
Average value: 0.824 J/cm Grade Count:26
 0.392266 - 1.27486 J/cm
@Thickness 3.20 - 6.40 mm
Average value: 0.824 J/cm Grade Count:26
Izod Impact, Notched (ISO) 6.00 - 58.0 kJ/m²Average value: 19.1 kJ/m² Grade Count:58
 6.00 - 41.0 kJ/m²
@Temperature -30.0 - -30.0 °C
Average value: 10.7 kJ/m² Grade Count:40
 9.00 - 9.00 kJ/m²
@Temperature -40.0 - -40.0 °C
Average value: 10.7 kJ/m² Grade Count:1
 9.00 - 9.00 kJ/m²
@Thickness 4.00 - 4.00 mm
Average value: 10.7 kJ/m² Grade Count:1
Izod Impact, Unnotched (ISO) 65.0 kJ/m² - NBAverage value: 87.5 kJ/m² Grade Count:17
 NB - NB
@Temperature -30.0 - -30.0 °C
Grade Count:2
Charpy Impact Unnotched 1.90 J/cm² - NBAverage value: 12.2 J/cm² Grade Count:58
 5.00 J/cm² - NB
@Temperature -40.0 - -30.0 °C
Average value: 10.6 J/cm² Grade Count:34
Charpy Impact, Notched 0.130 - 6.00 J/cm²Average value: 1.60 J/cm² Grade Count:115
 0.300 - 4.00 J/cm²
@Temperature -30.0 - -20.0 °C
Average value: 1.13 J/cm² Grade Count:49
Gardner Impact 2.71 - 36.2 JAverage value: 20.5 J Grade Count:3
Instrumented Impact Total Energy 21.0 - 55.0 JAverage value: 45.0 J Grade Count:9
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+14 - 6.00e+16 ohm-cmAverage value: 2.47e+15 ohm-cm Grade Count:56
Surface Resistance 1.00e+14 - 2.00e+17 ohmAverage value: 7.54e+15 ohm Grade Count:41
Dielectric Constant 2.70 - 3.20Average value: 3.02 Grade Count:30
Dielectric Strength 23.0 - 41.0 kV/mmAverage value: 33.1 kV/mm Grade Count:45
Dissipation Factor 0.00380 - 0.0900Average value: 0.0246 Grade Count:30
Arc Resistance 60.0 - 120 secAverage value: 90.0 sec Grade Count:11
Comparative Tracking Index 250 - 600 VAverage value: 593 V Grade Count:42
Hot Wire Ignition, HWI 7.00 - 60.0 secAverage value: 21.4 sec Grade Count:11
High Amp Arc Ignition, HAI 30.0 - 120 arcsAverage value: 110 arcs Grade Count:11
High Voltage Arc-Tracking Rate, HVTR 10.0 - 150 mm/minAverage value: 41.1 mm/min Grade Count:11
 
Thermal PropertiesOriginal ValueComments
CTE, linear 70.0 - 102 µm/m-°CAverage value: 83.2 µm/m-°C Grade Count:66
CTE, linear, Transverse to Flow 75.6 - 95.0 µm/m-°CAverage value: 85.2 µm/m-°C Grade Count:5
Thermal Conductivity 0.128 - 0.180 W/m-KAverage value: 0.166 W/m-K Grade Count:6
Maximum Service Temperature, Air 50.0 - 90.0 °CAverage value: 64.4 °C Grade Count:8
Hot Ball Pressure Test 95.0 - 120 °CAverage value: 103 °C Grade Count:11
Deflection Temperature at 0.46 MPa (66 psi) 89.0 - 122 °CAverage value: 104 °C Grade Count:118
Deflection Temperature at 1.8 MPa (264 psi) 76.7 - 130 °CAverage value: 96.4 °C Grade Count:211
Vicat Softening Point 97.0 - 165 °CAverage value: 110 °C Grade Count:171
Glass Transition Temp, Tg 108 - 127 °CAverage value: 116 °C Grade Count:9
UL RTI, Electrical 50.0 - 85.0 °CAverage value: 62.2 °C Grade Count:16
UL RTI, Mechanical with Impact 50.0 - 85.0 °CAverage value: 62.2 °C Grade Count:16
UL RTI, Mechanical without Impact 50.0 - 85.0 °CAverage value: 62.2 °C Grade Count:16
Flammability, UL94 HB - 5VAGrade Count:127
Glow Wire Test 650 - 700 °CAverage value: 682 °C Grade Count:17
 
Optical PropertiesOriginal ValueComments
Gloss 30.0 - 98.0 %Average value: 63.7 % Grade Count:14
 
Processing PropertiesOriginal ValueComments
Processing Temperature 180 - 270 °CAverage value: 239 °C Grade Count:38
Nozzle Temperature 180 - 270 °CAverage value: 239 °C Grade Count:44
Melt Temperature 180 - 274 °CAverage value: 226 °C Grade Count:101
Mold Temperature 30.0 - 100 °CAverage value: 62.2 °C Grade Count:135
Injection Velocity 200 - 240 mm/secAverage value: 237 mm/sec Grade Count:26
Drying Temperature 70.0 - 110 °CAverage value: 86.7 °C Grade Count:124
Injection Pressure 4.83 - 150 MPaAverage value: 49.3 MPa Grade Count:24

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled

O1102 / 77794

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.