MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Neopor® 5300 Expandable Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Expanded Polystyrene (EPS)

Material Notes: Description: Expandable polystyrene (EPS) containing uniformly distributed flame retardant (blowing agent: pentane).

Remarks: For the production of flame-retardant silver-gray foams having a considerably higher thermal-insulation capacity than the usual EPS insulating materials.

Applications: Block and molded parts.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.02 - 1.05 g/cc
Density 0.00310 g/ccPentane Blowing Agent Vapor (Heavier than air)
 0.600 g/cc
Bead Size 0.900 - 1.30 mm
 
Thermal PropertiesOriginal ValueComments
Softening Point 70.0 °Capprox
Decomposition Temperature >= 220 °C
Flash Point >= -56.0 °CPentane Blowing Agent
Ignition Temperature 285 °CPentane Blowing Agent; DIN 51794
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.50 %
 
Descriptive Properties
ColorBlack
Commercial StatusEurope
Sieve Analysis<0.8 mmmax 2%
 >1.4 mmmax 3%
 0.8 - 1.4 mmmax 95%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Styropor® BF 222 EPS
BASF Styropor® F 315 T-N Expandable Polystyrene
Overview of materials for Expanded Polystyrene (EPS)
BASF Styrodur® 3035 CS Extruded Rigid Polystyrene Foam (Europe)
BASF Styropor® P 240 EPS

PBASG0204 / 131837

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.