MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mid-Mountain Materials ARMATEX® SRS 28 Silica Fabric Coated with Silicone Rubber
Categories: Ceramic; Glass; Glass Fiber

Material Notes: ARMATEX® SRS 28 is a silica fabric coated with silicone rubber on one or both sides to a finished weight of 28 oz/sq yd. An ideal product for heavy duty protection of equipment and personnel, ARMATEX® SRS 28 has a higher temperature capability base fabric than traditional welding fabric, and the coated material has excellent abrasion resistance. Standard roll size: 50 LY.

Information provided by Mid-Mountain Materials

Key Words: MIL-I-24244
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 762 microns
Coating Weight 949 g/m²Ten Percent
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 450 °FCoating, Continuous
 1800 °FBase Fabric, Continuous
 
Descriptive Properties
Abrasion ResistanceExcellent
CertificationMIL-I-24244Base Fabric and Coated Fabric
CoatingCoated One or Both Sides
ColorRed
Flame ResistanceExcellent
Oil and Hydrocarbon ResistanceVery Good
Roll Length (ft)150
Tensile Strength (lbs/in)250
Width (in)28

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mid-Mountain Materials ARMATEX® SRS 40 Silica Fabric Impregnated with Silicone Rubber
Overview of materials for Silicone Rubber
3M Techical Ceramics Ekasic® C Silicone Carbide
AR-Glass Fiber, Generic
Celanese Celstran® PP-GF30-10 PP, 30% Glass Reinforced

CMID30a / 141223

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.