MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Elkem (Bluestar Silicones) CAF 33 Translucent Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: CAF 33 is a room temperature curing silicone elastomer:
  • ACETIC.
  • Non FLOWING.
  • BLACK, WHITE, TRANSLUCENT.
Example of Applications: This product is more specifically intended for industrial customers who use it for bonding/sealing in various applications:
  • Automotive: sealing on engines, bonding/sealing of sunroofs.
  • Domestic appliances: bonding of oven door brackets, sealing of washing machine tanks.
  • Aeronautic: miscellaneous bonding applications.
  • Industry: sealing of molding compartments, bonding of HCR silicones, sealing of industrial rotary machines (pumps, turbines, compressors).
Key Benefits:
  • Resists very high temperatures.
  • Good dielectric properties.
  • Adhesion to many surfaces.
  • High resistance to chemical agents.
  • Resistance to water and humidity.

Information provided by Bluestar Silicones

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 2.20 MPa319 psiNF ISO 37
Elongation at Break 500 %500 %NF ISO 37
 
Processing PropertiesMetricEnglishComments
Extrusion Rate 40.0 g/min40.0 g/minASTM C1183

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Rogers Arlon CP-375CR Silicone Rubber
Precision Polymer Engineering S40H Silicone Rubber
Overview of materials for Silicone Rubber
Momentive Performance Materials TSE 2267U Heat Cured Rubber - High Duro Translucent
BIW Silicone Rubber Extrusions, Standard Grades

PBLUST090 / 191066

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.