MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Angst+Pfister APSOplast® PPE GF30 Modified PPE + 30% glass fibre
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polyphenylene Ether, 30% Glass Filled

Material Notes: This PPE is reinforced with 30% glass fibre. In comparison with versions which are not reinforced, it has even better mechanical and thermal properties and higher dimensional stability. Moreover, it retains excellent electrical properties and resistance to hydrolysis.

Information provided by Angst + Pfister

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.30 g/ccDIN EN ISO 1183-1
Water Absorption 0.010 %
@Time 86400 sec
DIN EN ISO 62
 0.020 %
@Time 346000 sec
DIN EN ISO 62
Moisture Absorption 0.0400 %at saturation in standardized climate; DIN EN ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 87DIN EN ISO 868
Ball Indentation Hardness 200 MPaDIN EN ISO 2039-1
Tensile Strength, Yield 70.0 MPaDIN EN ISO 527
Elongation at Break 3.0 %DIN EN ISO 527
Modulus of Elasticity 4.50 GPaDIN EN ISO 527
Charpy Impact, Notched 5.00 kJ/m²DIN EN ISO 179-1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+15 ohmIEC 60093
Dielectric Strength 25.0 kV/mmIEC 60243
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 1.30 J/g-°C
Maximum Service Temperature, Air 100 °Clong term
 110 °Cshort term
Deflection Temperature at 1.8 MPa (264 psi) 135 °CDIN EN ISO 75 / A
Minimum Service Temperature, Air -20.0 °C
Flammability, UL94 HB
@Thickness 3.00 mm
 HB
@Thickness 6.00 mm
 
Descriptive Properties
Colorbeige

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PANGP051 / 250549

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.