MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Trinseo CALIBRE™ 2061-15 Polycarbonate Resin
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Overview: CALIBRE™ 2061-15 resin is suitable for steam and ethylene oxide sterilization required by the health care industry. CALIBRE 2061-15 provides excellent heat resistance, impact strength, and processability. CALIBRE 2061-6 resin is compliant with ISO 10993 (Biological Evaluation of Medical Devices) and is suitable for use in approved medical applications. This product contains mold release and is currently available in black color.

Main Characteristics:

  • ISO 10993
Applications:
  • Medical applications

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccISO 1183/A
Water Absorption 0.15 %
@Temperature 23.0 °C,
Time 86400 sec
ISO 62
Moisture Absorption at Equilibrium 0.32 %
@Temperature 23.0 °C
50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 in/inISO 294-4
Melt Flow 15 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 73ASTM D785
Hardness, Rockwell R 118ASTM D785
Tensile Strength at Break 68.0 MPaISO 527-2/50
 68.3 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 62.0 MPaISO 527-2/50
 62.1 MPa50 mm/min; ASTM D638
Elongation at Break 150 %50 mm/min; ASTM D638
Elongation at Yield 6.0 %50 mm/min; ASTM D638; ISO 527-2/50
Tensile Modulus 2210 MPa50 mm/min; ASTM D638
 2300 MPaISO 527-2/50
Flexural Strength 96.5 MPaMethod I (3 point load), 2.0 mm/min; ASTM D790
 98.0 MPa2.0 mm/min; ISO 178
Flexural Modulus 2400 MPa2.0 mm/min; ISO 178
 2410 MPaMethod I (3 point load), 2.0 mm/min; ASTM D790
Izod Impact, Notched 750 J/m
@Temperature 23.0 °C
ASTM D256
Izod Impact, Notched (ISO) 74.0 kJ/m²
@Temperature 23.0 °C
ISO 180/A
Izod Impact, Unnotched (ISO) NB
@Temperature 23.0 °C
ASTM D256
Charpy Impact, Notched 25.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
Tensile Impact Strength 378 kJ/m²ASTM D1822
Dart Drop, Total Energy 81.3 J3.39 m/sec; ASTM D3763
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.00e+17 ohm-cmASTM D257
Dielectric Constant 3.0
@Frequency 60 Hz
ASTM D150
 3.0
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 17.0 kV/mmASTM D149
 17.0 kV/mmIEC 60243-1
Dissipation Factor 0.0010
@Frequency 50 Hz
ASTM D150
 0.0020
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 68.0 µm/m-°C
@Temperature -40.0 - 82.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 139 °CAnnealed; ISO 75-2/B; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 120 °CUnannealed; ISO 75-2/A
 122 °CUnannealed; ASTM D648
 136 °CAnnealed; ASTM D648; ISO 75-2/A
Vicat Softening Point 143 °CISO 306/B50
 148 °C
@Load 5.10 kg
Rate A (50°C/h); ASTM D1525
Flammability, UL94 HB
@Thickness 1.50 mm
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.586ASTM D542; ISO 489
Haze 1.0 %ASTM D1003
Transmission, Visible 89 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trinseo CALIBRE™ 2061-22 Polycarbonate Resin
Overview of materials for Polycarbonate, Optical Grade
Dow Tyril® 100 SAN
Trinseo CALIBRE™ 5101-15 Polycarbonate Resin
Trinseo CALIBRE™ 5201-8 Polycarbonate Resin

PZZDWST027 / 142236

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.