MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Hifax TKS 672P 2066 Thermoplastic Olefinic Elastomer (TPO)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO)

Material Notes: Hifax polypropylene resins based on the Catalloy process are used in applications such as building and construction (e.g., single-ply roofing), industrial applications (e.g., wire and cable), and automotive industries. Hifax priovides good processability, excellent impact resistance, a broad range of stiffness from very soft to rigid products, high temperature resistance and low linear coefficient of thermal expansion.

Hifax TKS 672P 2066 is a medium melt flow, soft TPO compound based on LyondellBasell's proprietary Catalloy  process resin. Product is available as a customized color matched, pellet form. This grade is delivered in 2066 color version. Applications: Exterior Automotive Applications.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.910 g/cc0.0329 lb/in³ISO 1183-1A
Melt Flow 13 g/10 min
@Load 2.16 kg,
Temperature 230 °C
13 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 3535ISO 868
Tensile Strength, Yield 6.00 MPa870 psiISO 527-1,-2
Elongation at Break >= 400 %>= 400 %ISO 527-1,-2
Flexural Modulus 0.160 GPa23.2 ksiISO 178
Izod Impact, Notched (ISO)  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 180/1A
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 180/1A
 
Descriptive Properties
Processing MethodInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Canuck Compounders BK 8-8-4 Automotive Grade UV Stabilized Black Thermoplastic PolyOlefin (TPO)
Dow DT702 TPO
Borealis Daplen™ AK4504 TPO Compound

PEQT7305 / 218942

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.