MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lubrizol Estane® ZHF 80AT3 Thermoplastic Polyurethane, Flame Retardant  (discontinued **)
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyether Grade

Material Notes: Type: Estane® ZHF 80AT3 NAT 022 is an 80A non halogen, flame retardant, aromatic polyether-based thermoplastic polyurethane (TPU).

Appearance: Transparent spherical pellets

Features: Zero halogen

Uses: Wire and Cable

Available in Americas, Europe, Middle East, Africa, India and Asia

Information Provided by The Lubrizol Corporation

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.12 g/ccASTM D792
Maximum Moisture Content 0.050
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80ASTM D2240
Tensile Strength, Ultimate 6670 psiASTM D412
Elongation at Break 600 %ASTM D412
Taber Abrasion, mg/1000 Cycles 340
@Load 1.00 kg
H-18 wheel; ASTM D3389
Compression Set 20 %ASTM D395
Tensile Set 20 %ASTM D412
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 194 °FASTM D1525
Glass Transition Temp, Tg -36.0 °FDSC
Flammability, UL94 V-2
@Thickness 1.91 mm
 
Processing PropertiesOriginal ValueComments
Zone 1 185 °CExtrusion
Zone 2 185 °CExtrusion
Zone 3 190 °CExtrusion
Zone 4 185 °CExtrusion
Adapter Temperature 185 °C5, Extrusion
Die Temperature 180 °C6, Extrusion
 180 °C7, tip, Extrusion
Drying Temperature 100 °C
Dry Time 3.00 hour
Dew Point -40.0 °C
 
Component Elements PropertiesOriginal ValueComments
Loss on Ignition(%) 25 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Huntsman IROGRAN® A 95 P 5003 TPU-Polyether
Borealis LE6006 Polyethylene
BASF Elastollan® 1185 A FHF TPUR Flame Retardant Halogen Free
BASF Elastollan® 1154 D FHF TPUR Flame Retardant Halogen Free
Huntsman IROGRAN® A 85 P 5004 TPU-Polyether

PNOVEON597 / 121488

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.