MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Guang Dong LH-PS89 Antistatic PS
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Extrusion Grade

Material Notes: Application Field: Suitable for extruding and injecting tray, transfer plate, sheet, board the shell of electrical appliance, electronic parts

Feature: High impact strength, good toughness, molding processing ability, anticorrosion, low water absorption, dimension stability

Grade: Extrusion

Color: Natural color, color matching is available

Information provided by GuangDong LuHua New Material Technology Holding Co

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.00 - 1.20 g/cc1.00 - 1.20 g/ccGB1033-86
Melt Flow 1.9 g/10 min
@Load 2.16 kg,
Temperature 220 °C
1.9 g/10 min
@Load 4.76 lb,
Temperature 428 °F
ISO1133:1997
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 6565ISO2039/2-1981
Tensile Strength 18.0 MPa2610 psiISO527: 1996
Flexural Strength 30.0 MPa4350 psiISO178: 1993
Flexural Modulus 1.112 GPa161.3 ksiISO178: 1993
Tensile Impact Strength 4.80 kJ/m²2.28 ft-lb/in²ISO179: 2000
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1.00e+8 - 1.00e+9 ohm1.00e+8 - 1.00e+9 ohmGB/T1410
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 146 °C295 °FISO306: 1994
Heat Distortion Temperature 81.0 °C178 °FISO75-2:2003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGDON008 / 283956

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.