MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Clax Italia Perclax® Cast Acrylic
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Cast

Material Notes: Based on the most innovative and advanced technologies, Clax Italia’s Perclax® stands out for its outstanding optical properties, extreme purity, transparency, lightness, toughness and excellent light, aging, weathering and chemical reagent resistance, as well as tight dimensional tolerances.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccDIN 53479
Molecular Weight >= 3.00e+6 g/mol
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength >= 740 kg(f)/cm²DIN 53455
Elongation at Break >= 3 %DIN 53455
Modulus of Elasticity >= 3.14 GPaDIN 53457
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 70.0 °C
Vicat Softening Point >= 105 °CISO 306/B50
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.49DIN 53491
Haze <= 0.50 %ASTM D1003A
Transmission, Visible >= 92 %DIN 5036
 
Descriptive Properties
FlammabilityB2DIN 4192
Water Absorption30 mgISO 62, m.1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Acrylic, Cast
Clax Italia AQuariA® Cast Acrylic
Abatron TDS, AboThane 861019/8606-5 Acrylic/Polyurethane Enamel
Lucite International Perspex™ GS Acrylic Cast Sheet 000/0000
Plaskolite West Optix® CA-41 General Purpose Acrylic Resin

PCLAX990 / 192233

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.