MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
C.O.I.M. LARIPUR® LPR7025 Special Adipate Ester Polyurethane
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester, TP; Polyester Thermoplastic Elastomer; Polyurethane, TP

Material Notes: Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:
  • Excellent abrasion resistance
  • Great flexibility with constancy at temperature variations
  • Good compression resistance
  • Good water and light resistance
  • Good resistance to oils, fats and to many types of solvents

Series 25 Special Adipate Ester: These products are based on saturated polyesters. Products are based on saturated polyester. The features are similar to those of Series 20 but, by comparison, they are characterized by a higher resistance to hydrolysis and improved flexibility at low temperatures.
Information provided by P.A.T. Products, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.18 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 70ASTM D2240
Tensile Strength, Yield 43.2 MPaASTM D412
Elongation at Break 670 %ASTM D412
50% Modulus 0.00260 GPa
@Strain 50 %
ASTM D412
100% Modulus 0.00350 GPa
@Strain 100 %
ASTM D412
300% Modulus 0.0106 GPa
@Strain 300 %
ASTM D412
Tear Strength 76.0 kN/mASTM D624
Abrasion 30mm3, Abrasion Loss; DIN 53516
Compression Set 58 %
@Temperature 70.0 °C
Method B, 22 hours; ASTM D395
 23 %
@Temperature 23.0 °C,
Time 252000 sec
ASTM D395
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 60.0 °CASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
C.O.I.M. LARIPUR® LPR6518 Plasticized Ester Polyurethane
C.O.I.M. LARIPUR® LPR8025 Special Adipate Ester Polyurethane
C.O.I.M. LARIPUR® LPR4525 Special Adipate Ester Polyurethane
C.O.I.M. LARIPUR® LPR5520 Standard Adipate Ester Polyurethane
C.O.I.M. LARIPUR® LPR6515 Plasticized Ester Polyurethane

PCOIM006 / 28609

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.