MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Epsan Eplon 6 GFR 50 NC Q1F001 Polyamide 6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Polyamide 6, reinforced with 50% of glass fiber, heat stabilized, for injection molding.

Information provided by Epsan Plastik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.52 - 1.57 g/ccISO 1183
Moisture Absorption <= 0.20 %ISO 62
Linear Mold Shrinkage 0.0020 cm/cmParallel; ISO 294-4
 0.0030 cm/cmNormal; ISO 294-4
Ash 48 - 52 %ISO 3451
 
Mechanical PropertiesOriginal ValueComments
Tensile Stress 190 - 230 MPaISO 527-2
Elongation at Break 2.0 - 3.0 %ISO 527-2
Tensile Modulus 13000 - 15500 MPaISO 527-2
Flexural Strength 230 - 280 MPaISO 178
Flexural Modulus 11000 - 14500 MPaISO 178
Izod Impact, Notched (ISO) 14.0 - 20.0 kJ/m²ISO 180/1A
Charpy Impact, Notched 14.0 - 22.0 kJ/m²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 210 - 230 °CISO 3146
Flammability, UL94 HB
@Thickness 1.60 mm
UL-94
 
Processing PropertiesOriginal ValueComments
Processing Temperature 260 °CRecommended Injection Molding Temperature
Drying Temperature 80.0 °CAverage Drying Time is 2-4 hrs

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEPSAN096 / 186410

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.