MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kolon KOCETAL® TC704 Mineral Reinforced Acetal Resin
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Mineral Filled

Material Notes: Whisker reinforced, improved wear and dimensional property.

Applications: Dimensionally precise products.

Information provided by API-Kolon.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.55 g/ccASTM D792
Linear Mold Shrinkage 0.016 cm/cmASTM D955
Melt Flow 18 - 23 g/10 minASTM D1238
Ash 18 - 22 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 85ASTM D785
Tensile Strength 44.0 MPaASTM D638
Elongation at Break 5.0 %ASTM D638
Flexural Strength 83.0 MPaASTM D790
Flexural Modulus 4410 MPaASTM D790
Izod Impact, Notched 20.0 J/mASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmASTM D257
Surface Resistance 1.00e+16 ohmASTM D257
 
Thermal PropertiesOriginal ValueComments
Melting Point 166 °CASTM D1525
Flammability, UL94 HB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kolon KOCETAL® TC702 Mineral Reinforced Acetal Resin
Kolon KOCETAL® TC701 Mineral Reinforced Acetal Resin
PTS Trilac® ABS-HS5500 High Impact ABS Resin
Overview of materials for Acetal Copolymer, Unreinforced
Celanese Hostaform® XGC10 POM, 10% Glass Reinforced

PKOKZ917 / 122619

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.