MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
GEHR Plastics ECOGEHR® PLA-L Polylactic Acid  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: PLA-L is a blend of polylactide, some lignin, natural fatty acids and waxes. It combines good mechanical properties comparable with ABS, high rigidity, a tensile module of elasticity of up to 397 kpsi, good impact strength down to -22°F, good resistance to polar solvents, good thermal insulation and is approved for use with foodstuffs and toys.

Information provided by GEHR Plastics, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.25 g/ccISO 1183
Water Absorption at Saturation 0.50 %ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 75DIN 53505
Ball Indentation Hardness 105 MPaISO 2039
Tensile Strength at Break 22.8 MPaISO 527
Tensile Strength, Yield 51.0 MPaISO 527
Elongation at Break 11.8 %ISO 527
Elongation at Yield 2.5 %ISO 527
Modulus of Elasticity 2.70 GPaISO 527
Flexural Strength 70.0 MPaISO 178
Charpy Impact Unnotched 58.0 kJ/m²ISO 179
Charpy Impact, Notched 6.80 kJ/m²ISO 179
 
Thermal PropertiesOriginal ValueComments
CTE, linear 120 µm/m-°CDIN 53752
Thermal Conductivity 0.170 W/m-K
@Temperature 20.0 °C
Maximum Service Temperature, Air 60.0 °C
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °CISO 75
Vicat Softening Point 58.0 °CVST/A/50; ISO 306
 
Descriptive Properties
Bondabilityyes
Industrially BiodegradableYes
Renewable Content (%)80

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
GEHR Plastics ECO-GEHR® PLA-LF Polylactic Acid
Silicon Nitride
Overview of materials for Polylactic Acid (PLA) Biopolymer
Calcium Hydroxyapatite, Ca10(PO4)6(OH)2
Thoracic aorta Human Artery

PGEHR041 / 122024

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.