MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Guarniflon SC 1200 Polytetrafluoroethylene Seal
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: SC series is a superior and unique material for gasket (flat Sealing) applications. The overall benefits of Guarniflon SC series over that of both conventional PTFE and competitive PTFE/filler blends are found in the areas of environmental improvement (they are asbestos free) and overall cost saving. Main applications in the chemical, petrochemical, pharmaceutical, food, paper industries, etc.
Complies with FDA specifications.

Information provided by Guarniflon®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.24 g/cc0.0809 lb/in³ASTM D792
 
Chemical PropertiesMetricEnglishComments
Critical Pressure 80.0 bar60000 torrmax
 
Mechanical PropertiesMetricEnglishComments
Creep Strength 0.0300 MPa
@Temperature 23.0 °C
4.35 psi
@Temperature 73.4 °F
DIN 28090-2
 0.0500 MPa
@Temperature 150 °C,
Time 57600 sec
7.25 psi
@Temperature 302 °F,
Time 16.0 hour
DIN 28090-2
Compressive Modulus 0.00140 GPa
@Temperature 23.0 °C
0.203 ksi
@Temperature 73.4 °F
DIN 28090-2
 0.00740 GPa
@Temperature 150 °C,
Time 57600 sec
1.07 ksi
@Temperature 302 °F,
Time 16.0 hour
DIN 28090-2
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 260 °C500 °F
Minimum Service Temperature, Air -200 °C-328 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Descriptive Properties
ColorWhite, Grey
Compression Creep, MPa16150°C, 30 N/mm³
Leakage with Nitrogen, cm³/min0.01DIN 3535
Leakage, mg/s*m<.001DIN 28090-2
max P x T , bar °C12000
Recovery, mm0.09DIN 28090-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGUARN023 / 142756

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.