MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro DESMODUR® TD636 + BAYTEC® XL TMP-TIPA + PLASTICIZER V10 (SD6-40 Catalyst), 20 A Polyurethane, TDI- Ester
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes:

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.980 g/ccPLASTICIZER V10
 1.05 g/ccBAYTEC® XL TMP-TIPA
 1.19 g/cc
 1.19 g/ccDESMODUR® TD636
Viscosity 15 cPPLASTICIZER V10
 75 cPBAYTEC® XL TMP-TIPA
 2000 cPDESMODUR® TD636
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 20DIN 53505
 20
@Temperature 80.0 °C
DIN 53505
 28
@Temperature -5.00 °C
DIN 53505
Tensile Strength at Break 7.00 MPaDIN 53504
Tensile Stress at Strain 0.100 MPa
@Strain 10 %
DIN 53504
Elongation at Break 590 %DIN 53504
100% Modulus 0.000600 GPa
@Strain 100 %
DIN 53504
200% Modulus 0.000900 GPa
@Strain 200 %
DIN 53504
300% Modulus 0.00130 GPa
@Strain 300 %
DIN 53504
Resilience 35[%]; DIN 53512
Tear Strength 2.00 kN/mwith nick; ISO 34-1
 10.0 kN/mwithout nick; ISO 34-1
Compression Set 4.0 %
@Temperature 70.0 °C,
Time 79200 sec
ISO 815-1
 
Processing PropertiesOriginal ValueComments
Processing Temperature 80.0 °CPLASTICIZER V10
 80.0 °CDESMODUR® TD636
 90.0 °CBAYTEC® XL TMP-TIPA
Mold Temperature 110 °C
Pot Life 20.0 min
 
Descriptive Properties
AppearanceliquidPLASTICIZER V10
 solidDESMODUR® TD636
 solidBAYTEC® XL TMP-TIPA
Content0.8Catalyst SD6-40 % / total (by weight) (catalyst at the head)
 100Parts by weight of prepolymer
 3.4-3.8%NCO
 3.6Parts by weight of BAYTEC® XL TMP-TIPA
 50Parts by weight of PLASTICIZER V10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyester Grade
ExxonMobil Santoprene® 8211-25 Thermoplastic Elastomer
Barlog Plastics KEBAFLEX SG 25 A.1 TPE-S, Shore A25, natural
Barlog Plastics KEBAFLEX S 25 A.01 TPE-S, Shore A25, translucent
Avient Elastamax™ XL 0228-6 SBS-Based Thermoplastic Elastomer

PCOVEST0578 / 202361

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.