MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ITW Devcon Flexane® Rubber Repair / Castable Urethane High Performance Putty, Black
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS

Material Notes:

Information provided by ITW Devcon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0426 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 78Cured; ASTM D2240
Tensile Strength at Break 4500 psiASTM D412
Elongation at Break <= 600 %ASTM D412
Tear Strength 400 pliASTM D624
Taber Abrasion, mg/1000 Cycles 140H-18 wheel (1000 gram load)
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 350 V/milASTM D149
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 120 °Fwet
 180 °Fdry
Shrinkage 12 %Cured (shrinkage due to solvent loss); ASTM D2566
 
Processing PropertiesOriginal ValueComments
Cure Time 16.0 hourFunctional cure
Pot Life 10.0 min
@Temperature 23.9 °C
 
Descriptive Properties
Coverage per pound, in² @ 1/4" thickness94
Mix ratio by weight (Resin:Hardener)94:6

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ITW Devcon Rubber Repair / Castable Urethane Edge & Seal (T-35), Black
ITW Devcon Flexane® Rubber Repair / Castable Urethane 94 Liquid, Black
ITW Devcon Flexane® Rubber Repair / Castable Urethane Fast Cure, Black
ITW Devcon Flexane® Rubber Repair / Castable Urethane 80 Liquid, Black
ITW Devcon Flexane® Rubber Repair / Castable Urethane Brushable, Black

PITW01 / 48450

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.