MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Cosmic Plastics FARBOSET® 1115 Black Mineral Filled Epoxy Molding Compound
Categories: Polymer; Thermoset; Epoxy; Epoxy, Molded, Mineral Filled

Material Notes: Cosmic FARBOSET 1115 Black is a mineral filled epoxy molding compound featuring fast cure rates, and excellent hot strength. It is designed for the encapsulation of coils, transformers, bushings, switches and other electrical and electronic components requiring good hot rigidity in molding. This material is used extensively in injection and transfer molding.

Information provided by Cosmic Plastics Inc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 1.00 g/ccpowder
Density 2.04 g/cc
Water Absorption 0.026 %
@Time 86400 sec
Linear Mold Shrinkage 0.0050 in/in
Spiral Flow 71.0 cmEMMI 1-66A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 97
Tensile Strength at Break 12500 psi
Flexural Strength 18000 psi
Flexural Modulus 2.50e+6 psi
Compressive Strength 40000 psi
Izod Impact, Notched 0.400 ft-lb/in
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 5.00e+16 ohm-cm
Surface Resistance >= 1.00e+16 ohm
Dielectric Constant 4.5
@Frequency 1000 Hz
Dielectric Strength >= 400 V/milshort time 125 mil
Dissipation Factor 0.0070
@Frequency 1000 Hz
Dielectric Loss Index 0.032
@Frequency 1000 Hz
Arc Resistance 180 sec
 
Thermal PropertiesOriginal ValueComments
CTE, linear 17.8 µin/in-°FAlpha 1
 48.3 µin/in-°FAlpha 2
Thermal Conductivity 0.00320 cal cm/sec-cm²-°C
Maximum Service Temperature, Air 200 °C
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
Glass Transition Temp, Tg 130 °C
Flammability, UL94 V-0
@Thickness 1.59 mm
 
Processing PropertiesOriginal ValueComments
Mold Temperature 150 - 180 °C
Cure Time 1.00 - 3.00 min
@Temperature 150 °C
 30.0 sec
@Temperature 150 °C
Hot Plate
Shelf Life 0.0670 Month
@Temperature 35.0 °C
2 days
 0.250 Month
@Temperature 25.0 °C
1 week
 12.0 Month
@Temperature 5.00 °C
 
Descriptive Properties
Molding Pressure50-1000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Westlake Plastics Propylux® Polypropylene
Total 3629 Polypropylene, Injection Molding Grade
Sumitomo Bakelite Durez® 22257 Phenolic, Injection Grade
Overview of materials for Polypropylene, Molded
Mitsubishi Chemical Advanced Materials Ketron™ 1000 IM Injection Molded Unfilled Polyetheretherketone

PCOSM025 / 190807

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.