MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sax Polymers SAXLAC 320A Acrylonitrile Butadiene Styrene
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded

Material Notes: Saxalac 320A is an antistatic, high impact resistant and easy flowing ABS injection molding grade, characterized by good processability and high stiffness.

Mechanical property data tested at 50% RH.

Information provided by SAX Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.01 g/cc
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
Melt Flow 20 g/10 min
@Load 10.0 kg,
Temperature 220 °C
from MVR; ISO 1033
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 42.0 MPaISO 527-1
Elongation at Break 7.0 %ISO 527-1
Tensile Modulus 2200 MPaISO 527-1
Izod Impact, Notched (ISO) 10.0 kJ/m²
@Temperature -30.0 °C
ISO 180/1A
 25.0 kJ/m²
@Temperature 23.0 °C
ISO 180/1A
Izod Impact, Unnotched (ISO) 100 kJ/m²
@Temperature 23.0 °C
ISO 180
 100 kJ/m²
@Temperature -30.0 °C
ISO 180
Charpy Impact Unnotched 100 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
 100 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 10.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 24.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Hot Ball Pressure Test 95.0 °C
@Thickness 2.00 mm
IE/CEN 60335-1
Deflection Temperature at 1.8 MPa (264 psi) 82.0 °C80*10*4 s=60mm; ISO 75-1 a
Vicat Softening Point 95.0 °C50B; ISO 306
Flammability, UL94 HB
Glow Wire Flammability Index 650 °CIE/CEN 60695-2-12
 
Processing PropertiesOriginal ValueComments
Melt Temperature 220 - 260 °C
Mold Temperature 60.0 - 90.0 °C
Drying Temperature 80.0 °C
@Time 7200 - 14400 sec
Moisture Content <= 0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sax Polymers SAXLAC 310A Acrylonitrile Butadiene Styrene
Sax Polymers SAXLAC 310T Acrylonitrile Butadiene Styrene
Sax Polymers SAXLAC 320U Acrylonitrile Butadiene Styrene
Mitsubishi Iupilon® LSH 2010 Polycarbonate
Mitsubishi Iupilon® ELV 2010 Polycarbonate

PSAXP909 / 150858

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.