MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Gouda Refractories Pinnacle PP 4130H PP Impact Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Impact Modified; Molded/Extruded

Material Notes: Product Description: 35 melt flow, high impact copolymer for injection molding. Pinnacle Polymers Polypropylene 4130H is made via UNIPOL™ PP technology, which utilizes gas-phase fluidized bed reactors with a high activity catalyst system to ensure uniform physical properties and lot-to-lot consistency. This product is intended for injection molding of flooring, automotive, appliance, lawn and garden products, and industrial applications. Its high melt flow allows for quick filling of molds.
Features: Ultra high impact; Superior balance of stiffness and impact strength; UL Listed; Fast cycle-time
It is characterized not only by its easy flow, but also high impact at both room and sub-ambient conditions. Pinnacle’s 4130H polypropylene as marketed by Pinnacle Polymers Company, in natural, uncolored pellet form is covered under US FDA Food Contact Notification 864. As such, this polymer complies with the requirements of CFR Title 21 and can be used in contact with all food types under Conditions of Use A-H.

Availability: Europe; North America

Features: Fast Molding Cycle; Food Contact Acceptable; Good Color Stability; Good Processing Stability; High Flow; Impact Copolymer; Low Temperature Impact Resistance; Ultra High Impact Resistance

Agency Ratings: FDA FCN 864; FDA Food Contact A-H

Appearance: Natural Color

Form: Pellets

Processing Method: Injection Molding

Information provided by Pinnacle Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D1505
Linear Mold Shrinkage, Flow 0.014 cm/cmASTM D955
Melt Flow 35 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 3100 psi
@Thickness 3.20 mm
Injection Molded, Type I, 2.0 in/min; ASTM D638
Elongation at Break 6.0 %
@Temperature -17.7 °C
Injection Molded, Type I, 2.0 in/min; ASTM D638
Flexural Modulus 155000 psi
@Thickness 3.20 mm
1% Secant, Injection Molded, Type I, 0.05 in/min; ASTM D790A
Izod Impact, Notched >= 10.0 ft-lb/in
@Thickness 3.20 mm
Injection Molded, Type I; ASTM D256
 >= 24.7 ft-lb/in
@Thickness 3.20 mm
(Area) Injection Molded, Type I; ASTM D256
Izod Impact, Unnotched NB
@Thickness 3.20 mm
Injection Molded, Type I; ASTM D256
Gardner Impact 292 in-lb
@Temperature -30.0 °C
Geometry GC, Method G; ASTM D5420
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 210 °FUnannealed; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPINNA820 / 311513

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.