MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Process Technologies Inc EPDM Sanitary Gasket
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: EPDM (Ethylene Propylene Diene Monomer) This material is USP Class VI, FDA and 3A compliant. EPDM has very good water and steam resistance. Because of its polymer structure, this material does not offer strong resistance to oil, animal fat and most acids.

Information provided by Process Technologies Inc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 148.89 °C
Minimum Service Temperature, Air -34.44 °C
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes
 
Descriptive Properties
ColorBlack
 Red
 White
Compatibility for ChemicalsAcetoneExcellent
 AmmoniaExcellent
 Hydrochloric AcidLimited
 Hydrofluoric AcidLimited
 Hydrogen PeroxideNot Recommended
 Isopropyl AlcoholExcellent
 Nitric AcidGood
 Phosphoric AcidExcellent
 Sodium HydroxideExcellent
 Sodium HypochloriteGood
 Steam to 400ºF (204ºC)Limited
 Sulfuric AcidGood

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Vicone High Performance Rubber VicoSeal™ 003R-BK Rubber Vulcanized to Steel
Ethylene Propylene Rubber (EPM, EPDM)
Process Technologies Inc EPDM/Metal - Metal Detectable Sanitary Gasket
Trelleborg E550 EPDM Rubber
Seals Eastern 5053 Ethylene-Propylene Rubber

PPTI05 / 138117

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.