MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total PPR 8650 Polypropylene, Random Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: ATOFINA 8650 is a low melting, high ethylene random copolymer with improved color, optics and impact properties. The low melting point of ATOFINA 8650 makes it an excellent heat seal layer for oriented films. ATOFINA 8650 complies with FDA regulations Title 21 CFR Section 177. 1520(c) 3.1 and may be used under these provisions for food contact and packaging.

Application

ATOFINA 8650 is recommended for use in non-oriented film processes for manufacture of package films that require improved optical and impact properties and as a heat seal layer for oriented films.

Information provided provided by Total Petrochemicals.

Total Petrochemicals acquired former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.890 g/ccASTM D1505
Moisture Vapor Transmission 1.00 cc-mil/100 in²-24hr-atmASTM E96
Melt Flow 11 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 3000 psiASTM D882
1% Secant Modulus 70000 psiASTM D882
Dart Drop 240 g/milF50; ASTM D1709
Heat Seal Strength Initiation Temperature 124 °CMinimum seal strength is 200 g/in at 15 psi pressure and 1 sec.; ASTM D1709
 
Thermal PropertiesOriginal ValueComments
Melting Point 134 °CDSC-2 Differential Scanning Calorimeter
 
Optical PropertiesOriginal ValueComments
Haze 2.0 %ASTM D1003
Gloss 85 %45°; ASTM D2457
 
Compliance PropertiesOriginal ValueComments
FDA Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Baystar™ HL 323 MDPE Medium Density Polyethylene, Film Resin
LyondellBasell Hostalen PP XN125-P Polypropylene Copolymer
Total MDPE 3802 B Medium Density Polyethylene, Cable
Borealis RA7050-GN Polypropylene-Random-Copolymer for Pressure Pipe Systems
Borealis BB412E Polypropylene Block Copolymer for extrusion and injection

PFINAA076 / 38512

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.