MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Ensinger TECATEC PEEK MT CW50 black - Stock Shapes (rods, plates, tubes) Polyetheretherketone, Carbon Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Carbon Fiber Filled

Material Notes: Fillers: carbon fibers

Main features:

  • biocompatible
  • very high strength
  • high dimensional stability
  • very good sterilizable
  • inherent flame retardant
  • good heat deflection temperature
Target Industries:
  • mechanical engineering
  • medical technology

Information provided by Ensinger Composites.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.52 g/cc
Water Absorption 0.15 %
@Temperature 80.0 °C,
Time 173000 sec
DIN EN ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 500 MPa50mm/min, 50 N; average of warp and weft; DIN EN ISO 527-2
Tensile Modulus 51.7 GPa1mm/min; average of warp and weft; DIN EN ISO 527-2
Flexural Strength 750 MPa10mm/min, 10 N; average of warp and weft; DIN EN ISO 178
Flexural Modulus 48.0 GPa10mm/min, 10 N; average of warp and weft; DIN EN ISO 178
Compressive Modulus 24.0 GPa10mm/min, 5 N; thickness; EN ISO 604
 39.0 GPa10mm/min, 5 N; average of warp and weft; EN ISO 604
 
Thermal PropertiesOriginal ValueComments
CTE, linear 5.00 µm/m-°C
@Temperature 23.0 - 80.0 °C
fill; DIN EN ISO 11359-1;2
 5.00 µm/m-°C
@Temperature 23.0 - 80.0 °C
warp; DIN EN ISO 11359-1;2
 50.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
thickness; DIN EN ISO 11359-1;2
Melting Point 343 °CDIN EN ISO 11357
Maximum Service Temperature, Air 260 °Clong term
Glass Transition Temp, Tg 143 °CDIN EN ISO 11357
Flammability, UL94 V-0DIN IEC 60695-11-10
 
Descriptive Properties
Colorblack opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PENSIN508 / 287732

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.