MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Carbon Black, N-990 (MT)
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced; Rubber or Thermoset Elastomer (TSE)

Material Notes: Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and many other high performance polyurethane applications. Millathane 76 can be vulcanized by sulfur or peroxide cured systems.

Curing of Millathane®76 can easily be done with many types of peroxides. Millathane76 peroxide vulcanizates have superior compression set, greater heat stability, and are more resistant to reversion than sulfur cures..

All information provided by TSE Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5252
Tensile Strength 23.37 MPa3389 psi
Elongation at Break 710 %710 %
100% Modulus 1.32 MPa
@Strain 100 %
191 psi
@Strain 100 %
200% Modulus 2.35 MPa
@Strain 200 %
341 psi
@Strain 200 %
300% Modulus 4.11 MPa
@Strain 300 %
596 psi
@Strain 300 %
Tear Strength 45.0 kN/m257 pli
Taber Abrasion, mg/1000 Cycles 7.0
@Load 1.00 kg
7.0
@Load 2.20 lb
H-18 wheel
Compression Set 53.6 %
@Temperature 70.0 °C,
Time 79200 sec
53.6 %
@Temperature 158 °F,
Time 22.0 hour
 
Processing PropertiesMetricEnglishComments
Cure Time 11.0 min
@Temperature 154 °C
0.183 hour
@Temperature 309 °F
 
Descriptive Properties
Formulation as Tested0.5Zinc Stearate
 1Poly AC 617A
 1Thanecure® ZM
 1.5Sulfur
 10TP-95
 100Millathane 76
 2MBT
 20N-990
 4MBTS

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Carbon Black, N-326 (HS-HAF)
Northstar Polymers SAI-1 Low Viscosity Variable Ratio Polyurethane Gel
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.0 PHR MBT
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Carbon Black, N-220 (ISAF)
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Carbon Black, N-330 (HAF)

PMILL095 / 87139

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.