MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.00 - 1.65 g/cc0.0363 - 0.0596 lb/in³Average value: 1.17 g/cc Grade Count:270
Water Absorption 20.0 - 900 %20.0 - 900 %Average value: 214 % Grade Count:9
Loss On Ignition 28.0 - 32.0 %28.0 - 32.0 %Average value: 30.0 % Grade Count:5
Water Vapor Transmission 500 - 140000 g/m²/day32.2 - 9020 g/100 in²/dayAverage value: 27600 g/m²/day Grade Count:12
 300 - 6500 g/m²/day
@Temperature 38.0 - 38.0 °C
19.3 - 419 g/100 in²/day
@Temperature 100 - 100 °F
Average value: 4080 g/m²/day Grade Count:4
Viscosity 72000 - 72000 cP
@Temperature 204 - 204 °C
72000 - 72000 cP
@Temperature 399 - 399 °F
Average value: 72000 cP Grade Count:1
Maximum Moisture Content 0.0200 - 0.05000.0200 - 0.0500Average value: 0.0222 Grade Count:27
Linear Mold Shrinkage 0.00110 - 0.0150 cm/cm0.00110 - 0.0150 in/inAverage value: 0.00713 cm/cm Grade Count:95
Linear Mold Shrinkage, Transverse -0.00300 - 0.00900 cm/cm-0.00300 - 0.00900 in/inAverage value: 0.00457 cm/cm Grade Count:22
Melt Flow 3.00 - 150 g/10 min3.00 - 150 g/10 minAverage value: 39.6 g/10 min Grade Count:48
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 52.0 - 10052.0 - 100Average value: 85.2 Grade Count:198
Hardness, Shore D 22.0 - 95.022.0 - 95.0Average value: 55.8 Grade Count:117
Tensile Strength, Ultimate 1.72 - 90.0 MPa250 - 13100 psiAverage value: 39.7 MPa Grade Count:272
 28.42 - 51.7 MPa
@Temperature 75.0 - 75.0 °C
4122 - 7500 psi
@Temperature 167 - 167 °F
Average value: 39.2 MPa Grade Count:3
 28.42 - 51.7 MPa
@Time 0.000 - 4.84e+6 sec
4122 - 7500 psi
@Time 0.000 - 1340 hour
Average value: 39.2 MPa Grade Count:3
Tensile Strength, Yield 24.7 - 33.4 MPa3580 - 4840 psiAverage value: 29.4 MPa Grade Count:3
Elongation at Break 30.0 - 1040 %30.0 - 1040 %Average value: 532 % Grade Count:275
Modulus of Elasticity 0.0200 - 2.07 GPa2.90 - 300 ksiAverage value: 0.968 GPa Grade Count:16
Flexural Yield Strength 74.0 - 110 MPa10700 - 16000 psiAverage value: 95.1 MPa Grade Count:7
Flexural Modulus 0.00689 - 2.90 GPa1.00 - 421 ksiAverage value: 0.375 GPa Grade Count:96
Resilience 35.0 - 52.035.0 - 52.0Average value: 42.7 Grade Count:7
Rebound 30.0 - 58.0 %30.0 - 58.0 %Average value: 40.8 % Grade Count:18
Shear Modulus 0.00840 - 0.150 GPa1.22 - 21.8 ksiAverage value: 0.0519 GPa Grade Count:4
 0.0138 - 0.3656 GPa
@Temperature -50.0 - 0.000 °C
2.00 - 53.03 ksi
@Temperature -58.0 - 32.0 °F
Average value: 0.159 GPa Grade Count:1
Izod Impact, Notched 1.08 - 10.6 J/cm2.02 - 19.9 ft-lb/inAverage value: 3.58 J/cm Grade Count:7
Izod Impact, Notched (ISO) NBNBGrade Count:6
 32.0 - 100 kJ/m²
@Temperature -30.0 - -30.0 °C
15.2 - 47.6 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 60.5 kJ/m² Grade Count:4
Izod Impact, Unnotched (ISO) NBNBGrade Count:6
 42.0 - 120 kJ/m²
@Temperature -30.0 - -30.0 °C
20.0 - 57.1 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 75.8 kJ/m² Grade Count:4
Tear Strength 12.4 - 500 kN/m71.0 - 2850 pliAverage value: 99.6 kN/m Grade Count:194
Graves Tear Strength 21.0 - 167 kN/m120 - 950 pliAverage value: 80.4 kN/m Grade Count:33
Taber Abrasion, mg/1000 Cycles 3.00 - 3503.00 - 350Average value: 50.7 Grade Count:79
Compression Set 18.0 - 92.0 %18.0 - 92.0 %Average value: 39.0 % Grade Count:68
Tensile Set 6.00 - 130 %6.00 - 130 %Average value: 47.8 % Grade Count:50
 10.0 - 18.0 %
@Temperature 200 - 200 °C
10.0 - 18.0 %
@Temperature 392 - 392 °F
Average value: 14.3 % Grade Count:6
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 2.70e+9 - 1.00e+12 ohm-cm2.70e+9 - 1.00e+12 ohm-cmAverage value: 3.01e+11 ohm-cm Grade Count:4
Surface Resistance 1.50e+10 - 1.00e+12 ohm1.50e+10 - 1.00e+12 ohmAverage value: 3.04e+11 ohm Grade Count:4
Dielectric Constant 4.60 - 8.004.60 - 8.00Average value: 6.34 Grade Count:3
Dielectric Strength 39.0 - 49.0 kV/mm991 - 1240 kV/inAverage value: 44.7 kV/mm Grade Count:3
Dissipation Factor 0.0250 - 0.1210.0250 - 0.121Average value: 0.0560 Grade Count:3
Comparative Tracking Index 600 V600 VAverage value: 600 V Grade Count:7
 
Thermal PropertiesMetricEnglishComments
CTE, linear 88.7 - 175 µm/m-°C49.3 - 97.2 µin/in-°FAverage value: 153 µm/m-°C Grade Count:22
 88.7 - 170 µm/m-°C
@Temperature -80.0 - -30.0 °C
49.3 - 94.4 µin/in-°F
@Temperature -112 - -22.0 °F
Average value: 137 µm/m-°C Grade Count:6
Melting Point 110 - 284 °C230 - 543 °FAverage value: 156 °C Grade Count:38
Maximum Service Temperature, Air 100 °C212 °FAverage value: 100 °C Grade Count:6
Deflection Temperature at 0.46 MPa (66 psi) 65.0 - 132 °C149 - 270 °FAverage value: 103 °C Grade Count:7
Vicat Softening Point 58.0 - 145 °C136 - 293 °FAverage value: 102 °C Grade Count:66
Minimum Service Temperature, Air -50.0 °C-58.0 °FAverage value: -50.0 °C Grade Count:6
Brittleness Temperature -70.0 - -35.0 °C-94.0 - -31.0 °FAverage value: -63.2 °C Grade Count:11
Glass Transition Temp, Tg -70.0 - -17.0 °C-94.0 - 1.40 °FAverage value: -41.6 °C Grade Count:67
Clash Berg Stiffness Temperature -38.0 - 6.11 °C-36.4 - 43.0 °FAverage value: -8.59 °C Grade Count:3
Flammability, UL94 V-2 - V-0V-2 - V-0Grade Count:9
 
Optical PropertiesMetricEnglishComments
Haze 1.00 - 23.0 %1.00 - 23.0 %Average value: 5.61 % Grade Count:8
Transmission, Visible 90.0 %90.0 %Average value: 90.0 % Grade Count:8
 
Processing PropertiesMetricEnglishComments
Processing Temperature 130 - 221 °C266 - 430 °FAverage value: 192 °C Grade Count:34
Nozzle Temperature 19.3 - 510 °C66.7 - 950 °FAverage value: 203 °C Grade Count:78
Adapter Temperature 138 - 224 °C280 - 435 °FAverage value: 197 °C Grade Count:99
Die Temperature 138 - 229 °C280 - 445 °FAverage value: 196 °C Grade Count:103
Melt Temperature 121 - 246 °C250 - 475 °FAverage value: 192 °C Grade Count:139
Head Temperature 190 - 200 °C374 - 392 °FAverage value: 195 °C Grade Count:4
Mold Temperature 4.40 - 95.6 °C39.9 - 204 °FAverage value: 32.2 °C Grade Count:98
Drying Temperature 55.0 - 110 °C131 - 230 °FAverage value: 96.7 °C Grade Count:65
Moisture Content 0.0100 - 0.100 %0.0100 - 0.100 %Average value: 0.0800 % Grade Count:8
Dew Point -40.0 - -17.8 °C-40.0 - 0.000 °FAverage value: -37.4 °C Grade Count:29
Injection Pressure 2.00 - 7000 MPa290 - 1.02e+6 psiAverage value: 732 MPa Grade Count:5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade
Overview of materials for Thermoplastic Polyurethane, Elastomer, Glass Filled
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyester Grade
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyether Grade

O5032 / 78461

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.