MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Sumitomo Bakelite Sumikon® PM-TX115 Phenolic Resol
Categories: Polymer; Thermoset; Phenolic; Phenolic, Resole, Mineral Filled

Material Notes: SUMIKON PM-TX115 is a heat dissipative themoset molding compound. It is an electrical insulative based on a phenolic polymer. It is supplied in the form of granular/molding powder for molding.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.11 g/ccJIS K 6911
Water Absorption 0.13 %JIS K 6911
Linear Mold Shrinkage 0.0027 in/inJIS K 6911
 
Mechanical PropertiesOriginal ValueComments
Flexural Strength 115 MPaJIS K 6911
Flexural Modulus 19.0 GPaJIS K 6911
Charpy Impact, Notched 3.00 kJ/m²JIS K 6911
 
Electrical PropertiesOriginal ValueComments
Insulation Resistance 1.00e+11 ohmAfter boiling; JIS K 6911
 1.00e+12 ohmAs mold; JIS K 6911
Dielectric Strength 8.00 kV/mmJIS K 6911
Arc Resistance 188 secJIS K 6911
Comparative Tracking Index 200 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 1.50 W/m-KProbe method
Deflection Temperature at 1.8 MPa (264 psi) 246 °CJIS K 6911
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sumitomo Bakelite Sumikon® PM-TX230 Phenolic Novolac
Sumitomo Bakelite Sumikon® PM-TX110 Phenolic Resol
Overview of materials for Vinyl Ester Sheet Molding Compound
Sumitomo Bakelite Sumikon® PM-TX250 Phenolic Novolac
Sumitomo Bakelite Sumikon® PM-TX210 Phenolic Novolac

PSUMIT474 / 194279

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.