MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Telcar® TL-3954-62 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Vinyl (PVC); PVC, Wire and Cable Grade

Material Notes: Notes: Telcar TL-3954-62 is a general purpose thermoplastic elastomer designed for a variety of wire and cable applications, including cable jacketing and cable insulation. Telcar TL-3954-62 is a medium hardness, high density grade that is RoHS compliant grade that is suitable for both injection molding and extrusion.

Features: Filled; General Purpose; Good Mold Release: Good Moldability; Good Processability; High Density; High Specific Gravity; Low Flow; Medium Hardness

Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Construction Applications; Flexible Cord Jacketing; Industrial Applications; Industrial Cable Insulation; Terminal Cable Jacketing; Underground Power Cable; Wire and Cable Applications; Wire Jacketing

Forms: Pellets

Processing Method: Extrusion; Injection Molding

Injection Notes: Injection Rate: Moderate-Fast

Extrusion Notes: Screw Speed: 30 to 100 rpm

Information Provided by Teknor Apex

Key Words: TPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.18 g/ccASTM D792
Melt Flow 1.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 60
@Time 5.00 sec
Injection Molded; ASTM D2240
 62
@Time 1.00 sec
Injection Molded; ASTM D2240
Tensile Strength at Break 6.15 MPaFlow, Die C, 20 in/min; ASTM D412
 1130 psiAcross Flow, Die C, 20 in/min; ASTM D412
Tensile Stress at Strain 223 psi
@Strain 100 %
Across Flow, Die C, 20 in/min; ASTM D412
 301 psi
@Strain 100 %
Flow, Die C, 20 in/min; ASTM D412
 351 psi
@Strain 300 %
Across Flow, Die C, 20 in/min; ASTM D412
 433 psi
@Strain 300 %
Flow, Die C, 20 in/min; ASTM D412
Elongation at Break 670 %Flow, Die C, 20 in/min; ASTM D412
 730 %Across Flow, Die C, 20 in/min; ASTM D412
Tear Strength 149 pliFlow, Die C, 20 in/min; ASTM D624
 157 pliAcross Flow, Die C, 20 in/min; ASTM D624
Compression Set 26 %
@Temperature 22.8 °C,
Time 79200 sec
Type 1; ASTM D395B
 46 %
@Temperature 70.0 °C,
Time 79200 sec
Type 1; ASTM D395B
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= -76.0 °FASTM D746
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 340 - 380 °F
Middle Barrel Temperature 350 - 390 °F
Front Barrel Temperature 360 - 400 °F
Nozzle Temperature 370 - 410 °F
Zone 1 330 - 370 °F
Zone 2 340 - 380 °F
Zone 3 350 - 390 °F
Zone 4 350 - 390 °C
Zone 5 360 - 400 °F
Die Temperature 374 - 410 °F
Melt Temperature 370 - 410 °FProcessing Temperature
Mold Temperature 77.0 - 150 °F
Injection Pressure 200 - 1000 psi
Back Pressure 25.0 - 50.0 psi
Cushion 0.150 - 1.00 in
Screw Speed 50 - 100 rpm
 
Descriptive Properties
AppearanceOpaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Teknor Apex Sarlink® 4380 Thermoplastic Elastomer
Overview of materials for PVC, Flexible Grade
Avient ProFlex™ MB NP70/30 Nitrile/PVC Elastomer (NBR/PVC) Compound
Armacell Ensolite™ AG2 Continuous Rolls/Sheets, PVC/NBR
AlphaGary Garaflex™ E X 00-207F UV-FG LCF Vinyl Thermoplastic Elastomer

PTEKNP500 / 129581

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.