MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Westlake Epolene® C-26 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer, Maleation Processed
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Product Description: Epolene C-26 is a maleic anhydride grafted polyethylene coupling agent for polyethylene (PE) composites. The polar functionality and molecular weight are optimized to provide balanced attraction between PE and reinforcements / fillers like glass, wood, minerals, and metals. Epolene C-26 Polymers are products of Westlake Chemical Corporation and are protected under one or more of the following U.S. patents: 5,955,547 and 6,046,279; and their foreign equivalents.
    Key Attributes:
  • Balances attraction between polar fillers/reinforcements and non polar polymers
  • Coupling agent for PE composites
  • Maleic anhydride grafted polyethylene(PE)
    Application/Uses:
  • Automotive OEM
  • Building and Construction
  • Rubber and Plastic Modification

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.910 - 0.920 g/cc
Brookfield Viscosity 8.0 cP
@Load 0.00000220 kg,
Temperature 190 °C
Molecular Weight 65000 g/molMw
Melt Flow 2.0 - 10 g/10 minPTM-008
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 8.0ASTM D1386
 
Thermal PropertiesOriginal ValueComments
Ring & Ball Softening Point 122 °CDSC Tm; ASTM E28
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 11VCC-099
 
Descriptive Properties
Penetration Hardness<1 dmmASTM D5, Needle under 100-g load for 5s @ 25 deg C, tenths of mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Westlake Epolene® C-19 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer, Maleation Processed
Westlake Epolene® E-20 Emulsifiable - Oxidized Low Molecular Weight Polyethylene Polymer
LyondellBasell Plexar® PX2250 Extrudable Tie-Layer Resin, Anhydride Modified HDPE
Westlake Epolene® C-18 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer, Maleation Processed, Chemically Modified
Westlake Epolene® E-10 Emulsifiable - Oxidized Low Molecular Weight Polyethylene Polymer

PWESF9025 / 106862

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.