MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total Lumicene® mPE M 4041 UV Metallocene Polyethylene, Rotomolding
Categories: Polymer; Thermoplastic; Polyethylene (PE); Medium Density (MDPE); Medium Density Polyethylene (MDPE), Rotational Molded

Material Notes: Lumicene® mPE M 4041 UV is a new generation metallocene medium density polyethylene with hexene as comonomer.

Lumicene® mPE M 4041 UV is intended for the manufacture of rotomolded items.

Lumicene® mPE M 4041 UV is a natural grade available in pellets form.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.940 g/ccISO 1183
Melt Flow 4.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133/D
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 21.0 MPaISO 527-2
Tensile Strength, Yield 21.0 MPaISO 527-2
Elongation at Break >= 800 %ISO 527-2
Elongation at Yield 11 %ISO 527-2
Flexural Modulus 730 MPaISO 178
Charpy Impact, Notched >= 150 kJ/m²
@Temperature 23.0 °C
ISO 179-1
 >= 150 kJ/m²
@Temperature -30.0 °C
ISO 179-1
 
Thermal PropertiesOriginal ValueComments
Melting Point 126 °CISO 11357

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Baystar™ Lumicene® mPE M 3581 UV Metallocene Medium Density Polyethylene Rotational Molding Resin – Pellet Form
Total Lumicene® mPE M 4707 EP Metallocene Polyethylene, Blown Film
Total Lumicene® mPE M 5220 High Density Polyethylene, Blow Molding
Total Lumicene® MR10MX0 Metallocene Random Copolymer Polypropylene, Injection Molding and Injection Blow Molding
Total Lumicene® mPE M 3509 Medium Density Polyethylene, Blow Molding

PTOTAL779 / 130504

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.