MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lubrizol LifeSciences Tecoflex® MG-8020-B20 TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Rigid RADIOPAQUE GRADE (20% loading of barium sulfate), Medical Grade Rigid Aliphatic TPUs

Features: Do not yellow, with high mechanical properties, radiopacity, and can be color-matched

Process: Injection Molding

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.30 g/ccASTM D792
Linear Mold Shrinkage 0.011 in/inASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 75ASTM D2240
Tensile Strength, Ultimate 7500 psiASTM D412
Elongation at Break 45 %ASTM D412
Flexural Modulus 185000 psiASTM D790

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol LifeSciences Carbothane® PC-3575A TPU – Clear Aliphatic
Lubrizol LifeSciences Tecoflex® EG-80A TPU - Clear
Lubrizol LifeSciences Tecoflex® MG-8020 TPU - Clear
Arkema Pebax® Rnew® 80R53 SP 02 TPA
Arkema Pebax® Rnew® 30R51 SA 01 TPA

PLUBR9063 / 203630

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.