MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Resistalloy International Resistalloy 6015 Nickel Chromium Electrical Resistance Alloy
Categories: Metal; Electronic/Magnetic Alloy; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small laboratory kilns to heavy-duty heat-treatment furnaces under all types of atmospheres. Available as wire and strip. Slightly magnetic.

Information provided by Resistalloy International Limited.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.20 g/cc0.296 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 180180
Tensile Strength, Ultimate 750 MPa109000 psi
 100 MPa
@Temperature 900 °C
14500 psi
@Temperature 1650 °F
Tensile Strength, Yield 450 MPa65300 psi
Elongation at Break 25 - 30 %
@Thickness 50.0 mm
25 - 30 %
@Thickness 1.97 in
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000111 ohm-cm0.000111 ohm-cmTemperature Factor is 1.10 at 800°C (1470°F). Temperature Factor is 1.11 at 1000°C (1830°F). Temperature Factor is 1.13 at 1200°C (2190°F).
 
Thermal PropertiesMetricEnglishComments
CTE, linear  14.0 µm/m-°C
@Temperature 20.0 - 250 °C
7.78 µin/in-°F
@Temperature 68.0 - 482 °F
 15.0 µm/m-°C
@Temperature 20.0 - 500 °C
8.33 µin/in-°F
@Temperature 68.0 - 932 °F
 17.0 µm/m-°C
@Temperature 20.0 - 1000 °C
9.44 µin/in-°F
@Temperature 68.0 - 1830 °F
Specific Heat Capacity 0.460 J/g-°C0.110 BTU/lb-°F
Thermal Conductivity 13.0 W/m-K90.2 BTU-in/hr-ft²-°F
Melting Point 1390 °C2530 °F
Maximum Service Temperature, Air 1150 °C2100 °F
 
Optical PropertiesMetricEnglishComments
Emissivity (0-1) 0.880.88Fully Oxidized
 
Component Elements PropertiesMetricEnglishComments
Chromium, Cr 15 %15 %
Iron, Fe 25 %25 %
Nickel, Ni 60 %60 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Resistalloy International Fecralloy™ 145 Electrical Resistance Steel
Resistalloy International Resistalloy 3718 Nickel Chromium Electrical Resistance Alloy
Resistalloy International Fecralloy™ 134 Electrical Resistance Steel
Resistalloy International Fecralloy™ 135 Electrical Resistance Steel
Resistalloy International Fecralloy™ Electrical Resistance Steel

NRESIST1 / 18828

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.