MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Domo TECHNYL® A 218 V35 Black 21NHFE PA66, 35% glass fiber, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Glass Fiber Filled

Material Notes: Description: TECHNYL® A 218 V35 BLACK 21NHFE is polyamide 6.6, high flow, reinforced with 35% glass fiber, heat stabilized, for injection molding. This product is available in black color.

Benefits: This product has enhanced molding behaviors and better surface aspect. It offers an excellent combination between thermal and mechanical properties. This grade is ideal for use in the automotive industry for engine components. This grade is ideal for Mucell® injection molding technology.

Available in: Asia Pacific, Europe, Latin America and North America

Regulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications

Applications: This grade is suitable for all kind of applications in automotive (pulleys, Inlet manifolds, air-ducts, engine covers) and non automotive that required a good balanced behavior between surface aspect, thermal and mechanical behavior.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.41 g/ccISO 1183/A
Water Absorption 0.75 %
@Temperature 23.0 °C,
Time 86400 sec
ISO 62
Viscosity 130 cP
@Shear Rate 100 1/s,
Temperature 275 °C
 300 cP
@Shear Rate 10 1/s,
Temperature 275 °C
Linear Mold Shrinkage 0.0060 cm/cmIsotropy
Linear Mold Shrinkage, Flow 0.0045 cm/cm
Linear Mold Shrinkage, Transverse 0.0075 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 200 MPaISO 527 Type 1A
Tensile Stress at Strain 110 MPa
@Strain 1 %
 180 MPa
@Strain 2 %
 205 MPa
@Strain 3 %
Elongation at Break 3.0 %ISO 527 Type 1A
Tensile Modulus 11100 MPaISO 527 Type 1A
Flexural Strength 280 MPaISO 178
Flexural Modulus 9500 MPaISO 178
Charpy Impact Unnotched 80.0 kJ/m²ISO 179/1eU
Charpy Impact, Notched 11.0 kJ/m²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 263 °CISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 255 °CISO 75/Af
 
Processing PropertiesOriginal ValueComments
Feed Temperature 265 - 275 °C
Mold Temperature 60.0 - 80.0 °C
Drying Temperature 80.0 °C
Moisture Content <= 0.20 %
 
Descriptive Properties
Compression Zone270-280°C
Mixing Zone280-290°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo TECHNYL® A 218 V35 Black 21NHFE PA66, 35% glass fiber, Conditioned
Celanese Zytel® 70G30HSLR NC010 PA66-GF30
DuPont Mobility and Materials Zytel® 7301 NC010 PA6
Domo TECHNYL® A 218 V35 PA66, 35% glass fiber, DRY
Domo TECHNYL® A 238 Black 21 N PA66, DRY

PRHOD641 / 137872

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.