MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NOVA Chemicals NOVAPOL® TR-0338-UI LLDPE Rotational Molding Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade

Material Notes:

Hexene Copolymer

Features:

  • Excellent low temperature impact properties
  • Excellent ESCR
  • Good stiffness
  • Wide processing window
  • NSF listed for Standards #24, 51, 61
  • UL94 HB

Additives:

  • Processing antioxidant
  • UV stabilizer

Applications:

  • General purpose custom molding
  • Chemical containers
  • IBCs
  • Fish boxes
  • Septic tanks
  • Agricultural storage tanks

United States: NOVAPOL TR-0338-UI(UIG) resin complies with the specifications contained in the U.S. Food and Drug Administration (FDA) regulation 21 CFR 177.1520 for olefin polymers, para. (c) 3.2a, and may thus be used in the United States as an article or component of an article intended for use in contact with food. This resin is subject to the specific limitations that it may contact food only in articles having a volume of at least 18.9 L (5 gal. U.S.), only at temperatures of 150°F and below, and may not be used to hold ready-prepared foods intended to be reheated in the container at time of use (21 CFR 176.170(c) Table 2, conditions of use D–G).

NOVA Chemicals polyethylene resins are biologically and chemically inert.

Information provided by NOVA Chemicals®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.938 g/ccASTM D 792
ESCR 100% Igepal® >= 1000 hour
@Temperature 50.0 °C
F50, Condition A and B. From compression molded specimens.; ASTM D 1693
Melt Index of Compound 3.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D 1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 19.4 MPa
@Thickness 1.91 mm
Type IV Specimen, 2" (50.8 mm) per minute test speed; ASTM D 638
Elongation at Yield 11 %
@Thickness 1.91 mm
Type IV specimen, 2" (50.8 mm) per minute test speed; ASTM D 638
Flexural Modulus 760 MPa
@Strain 1 %
ASTM D 790
Impact Test 70.0 J
@Thickness 3.17 mm,
Temperature -40.0 °C
ARM Low Temperature Impact; ARM Method
 220 J
@Thickness 6.35 mm,
Temperature -40.0 °C
ARM Low Temperature Impact; ARM Method
 
Thermal PropertiesOriginal ValueComments
Melting Point 125 °C(DSC)
Heat Distortion Temperature 43.0 °C
@Pressure 1.82 MPa
ASTM D 648
 60.0 °C
@Pressure 0.455 MPa
ASTM D 648
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chevron Phillips Marlex® HMN TR-938/938G Polyethylene; MDPE
ExxonMobil LL 8460 Rotational Molding Resin
Nexeo® HIVAL® 106033 Linear Low Density Polyethylene
Celanese Ateva® 1821A Film Ethylene Vinyl Acetate Copolymer Film
Nexeo® HIVAL® 103538 Linear Low Density Polyethylene

PNOVB046 / 194654

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.