MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
PoolKemie Resin PU 087 Casting Polyurethane system
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Introduction: Two component odorless polyurethane system with separate filler. The filler can be added in the suggested or in a different ratio depending on the application and on the required thickness of the casting. Very good detail reproduction, fast cure, low exothermic reaction, low shrinkage. The use of AL 3-H filler (mix ratio 100:100:150) allows production of components with lower specific weight.

Application: Foundry patterns, copy models, negatives, fast reproductions. Prototypes, short runs of casting components. Vacuum thermoforming tooling.

Component A: PU 087
Component B: PUH 887
Component C: AL 3-H

Information provided by Poolkemie

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.960 - 0.980 g/ccresin; ASTM D 1475
 1.09 - 1.12 g/cchardener; ASTM D 1475
Viscosity 40 - 50 cPA + B, Initial
 2500 - 3500 cPA + B + C, Initial
 
Processing PropertiesOriginal ValueComments
Cure Time 6.00 - 7.00 minDemoulding time, A + B + C, 15 ml, 6 mm
 30.0 - 45.0 minDemoulding time, A + B, 15 ml, 6 mm
 2.00 - 4.00 hour
@Temperature 60.0 °C
Post-curing, A + B
 2.00 - 4.00 hour
@Temperature 60.0 °C
Post-curing, A + B + C
Pot Life 3.00 - 4.00 minA + B, 100 ml, 40 mm
 5.00 - 6.00 minA + B + C, 100 ml, 40 mm
Gel Time 4.00 - 5.00 minA + B, 15 ml, 6 mm
 45.0 - 60.0 minA + B + C, 15 ml, 6 mm
 
Descriptive Properties
ColorPale YellowHardener
 WhiteResin
Exothermic peak30-40°CA + B + C, 100 mi, 40 mm
 80-90°CA + B, 100 mi, 40 mm
Mixing ratio100 gA + B, by weight
 100 gA + B + C, by weight
 100:100
 300 gA + B + C, by volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPOOLK038 / 318517

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.