MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Gromax 1140LH TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Product Description: 1140LH is Low modulus grade with nominal Durometer hardness of 40D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like injection molding and extrusion molding grade.

Characteristics:

  • Excellent low modulus for injection molding and extrusion molding grade.
  • Excellent flexibility and fatigue resistance.
  • Excellent creep resistance.
  • Excellent low shrinkage and higher melting temperature

    Information provided by Gromax Enterprises Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.146 g/cc1.146 g/ccISO 1183
Moisture Absorption 0.500 %
@Time 86400 sec
0.500 %
@Time 24.0 hour
ISO 62
Linear Mold Shrinkage 0.065 cm/cm0.065 in/inISO 294-4
Melt Flow 30 g/10 min
@Load 2.16 kg,
Temperature 230 °C
30 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4040ISO 868
Tensile Strength 19.6 MPa2840 psiISO 527
Elongation at Break 460 %460 %ISO 527
Tensile Modulus 0.115 GPa16.7 ksiISO 527
Flexural Modulus 0.113 GPa16.4 ksiISO 178
Charpy Impact, Notched NBNBISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 4.88e+12 ohm-cm4.88e+12 ohm-cmIEC 60093
Surface Resistance 8.10e+13 ohm8.10e+13 ohmIEC 60093
Dielectric Strength 16.4 kV/mm
@Thickness 2.00 mm
417 kV/in
@Thickness 0.0787 in
IEC 60243-1
 
Thermal PropertiesMetricEnglishComments
Melting Point 207 °C405 °FISO 3146C
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 210 - 220 °C410 - 428 °F
Middle Barrel Temperature 220 - 250 °C428 - 482 °F
Front Barrel Temperature 220 - 250 °C428 - 482 °F
Nozzle Temperature 220 - 250 °C428 - 482 °F
Mold Temperature 20.0 - 50.0 °C68.0 - 122 °F
Injection Pressure 30.0 - 100 MPa
@Time 2.00 - 10.0 sec
4350 - 14500 psi
@Time 0.000556 - 0.00278 hour
Hold Pressure 5.00 - 40.0 MPa
@Time 10.0 - 30.0 sec
725 - 5800 psi
@Time 0.00278 - 0.00833 hour
Screw Speed 40 - 80 rpm40 - 80 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGROM049 / 147862

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.